| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256-93a |
|
Multibase Multi-Pro® 4005 M I Medium Impact 40% Filler Content Polypropylene
Multi-Pro 4005 M I is a chemically coupled reinforced polypropylene compound featuring high flex modulus and high impact under retention of the heat resistance properties. The product is designed f..
|
|||
| Izod Impact, Notched |
0.480
J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.899
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
|
PolyOne LubriOne™ ATH-XC-361E Acetal (POM) Homopolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
NCMT NanoPAC™ G2050H High Performance Polypropylene Nanocomposite
Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256-93a |
|
Multibase Multi-Pro® 3019 CXUW High Gloss 30% TiO2 Filler Content Polypropylene
Multi-Pro 3019 CXUW is a mineral reinforced polypropylene compound exhibiting high stiffness and impact characteristics. This material was specially formulated with UV stabilization for outdoor app..
|
|||
| Izod Impact, Notched |
0.480
J/cm @Thickness 3.18 mm |
0.899
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
LNP Stat-Kon® OC-1006 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
(Unverified Data**)
Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h..
|
|||
| Izod Impact, Notched | 0.480 - 0.530 J/cm | 0.899 - 0.993 ft-lb/in | ASTM D256A |
|
DSM Somos® 9120 Epoxy Photopolymer
(Unverified Data**)
DescriptionDSM Somos® 9120 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p..
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
Kolon KOCETAL® CB301 Conductive Grade Acetal Resin
Conductive grade. Applications: Conductive products. Information provided by API-Kolon.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP KP004AXC Acetal Homopolymer
LNP LUBRICOMP* KP004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics ULTEM 2110 PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Izod Impact, Notched |
0.480
J/cm @Temperature -30.0 °C |
0.899
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| Izod Impact, Notched |
0.480
J/cm @Temperature 23.0 °C |
0.899
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES
LNP* THERMOCOMP* JF003XXZ is a compound based on Polyethersulfone resin containing 15% Glass Fiber.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP PH1000A PA 6
LNP THERMOCOMP* PH1000A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 (Asia Pacific)
LNP* Thermocomp* RF0069SZ is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
|
|||
| Izod Impact, Notched |
0.480
J/cm @Temperature 23.0 °C |
0.899
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Lubricomp LL003E PEEK
LNP* Lubricomp* LL003E is a compound based on Polyetheretherketone (PEEK) containing PTFE. Characteristics of this grade are: Easy Molding and Internally Lubricated.This data was supplied by SABIC..
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® 451E PBT (Asia Pacific)
20% GR. Easy flow version of VALOX 451.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP
LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Izod Impact, Notched |
0.480
J/cm @Temperature 23.0 °C |
0.899
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Thermocomp OF003A PPS (Asia Pacific)
LNP* Thermocomp* OF003A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer
DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene
DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ FPP 1477 Mineral Filled, General-Purpose Polypropylene
DescriptionPolyfort® FPP 1477 is a 20% mineral filled, general-purpose polypropylene.Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 0.480 - 0.530 J/cm | 0.899 - 0.993 ft-lb/in | UV Postcure; ASTM D256A |
|
DSM Somos® 9120
The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp..
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Voloy® 685 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.48% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod..
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
Ashley Polymers Ashlene® 197-N2 Acetal
A general purpose, very low viscosity, in natural.Data provided by the manufacturer
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Comtuf® 152 Polypropylene, Mineral Reinforced, Impact Modified
Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i..
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Lubrilon® 606 Nylon 6/6, PTFE Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
|
|||
| Izod Impact, Notched |
0.480
J/cm @Thickness 3.18 mm |
0.899
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
LNP Lubricomp® OCL-4534 EM Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant
(discont
Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g..
|
|||
| Izod Impact, Notched |
0.480
J/cm @Thickness 6.35 mm |
0.899
ft-lb/in @Thickness 0.250 in |
ASTM D256 |
|
PolyOne Edgetek® ES-06CF-09GF/000 RED Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications
&
Data provided by PolyOne.
|
|||
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester, TP (Asia Pacific)
LNP* THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Mineral, Glass Fiber. Added features of this material include: Flame Retardant.
|
|||