Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.600 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.600 J/cm
<br>@Thickness 4.00 mm,<br> Temperature 23.0 °C
1.12 ft-lb/in
<br>@Thickness 0.157 in,<br> Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
Izod Impact, Notched 0.600 J/cm
<br>@Temperature -30.0 °C
1.12 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Cycoloy® CM6240 PC+ABS (Asia Pacific)
CYCOLOY CM6240 resin is a flame retardant PC/ABS blend featuring balanced properties of high modulus, good flow and ductility. It is of Br- & Cl-free flame retardant systems intended to meet thin wa..
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant, High Flow
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
fiber
Reliance Industries Polypropylene Random Copolymer
Typical properties of Reliance - Repol Polypropylene gradesInformation provided by Reliance Industries
Izod Impact, Notched 0.600 J/cm
<br>@Thickness 4.00 mm,<br> Temperature 23.0 °C
1.12 ft-lb/in
<br>@Thickness 0.157 in,<br> Temperature 73.4 °F
Notched V 10 mm; ASTM D256
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound &nbsp;(discontinued **)
Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate..
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
Molded; ASTM D256
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 ..
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
LG Chemical LUCEL FW-715C Friction and Wear Resistant POM, Polymeric Wear Additive, CaCo3 Filled, Low Warpage, Antistatic
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
LG Chemical LUCEL N127-02 General Purpose POM, Unreinforced, Externally Lubricated, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Izod Impact, Notched 0.600 J/cm
<br>@Temperature -30.0 °C
1.12 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Xenoy® 1760E PBT+PC
11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin.
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
SPS Guang Zhou FILLMAâ„¢ 5002F30B Mineral Filled Polypropylene
Characteristic: 30%wt of Sulfate Barium filled, high gloss, high heat resistanceApplications: Household appliance partsInformation Provided by SPS (Guang Zhou) Ltd.
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East)
Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl ..
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT
LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber.
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene
DescriptionPolyfort® FXP 1943 is a 20% CAC03 and glass fiber hybrid copolymer polypropylene product. Information provided by A. Schulman.
Izod Impact, Notched 0.600 J/cm
<br>@Temperature 23.0 °C
1.12 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram PlusTek PA602 Nylon 6.6, Heat Stabilized
Heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 0.600 J/cm
<br>@Temperature 23.0 °C
1.12 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram PlusTek PB300G3 Nylon 6, 15% Glass Fiber
15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ISO 180
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Izod Impact, Notched >= 0.600 J/cm
<br>@Temperature 23.0 °C
>= 1.12 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram RamTal RM2309 Acetal, Injection Molding
Acetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer
DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman.
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene
DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman.
Izod Impact, Notched 0.600 J/cm
<br>@Temperature 23.0 °C
1.12 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram RamTal PM1609 Acetal, Molybdenum Disulfide Filled
Molybdenum disulfide filled polyacetal for injection molding applications.Information provided by Polyram Ram On Ind.
Izod Impact, Notched 0.600 J/cm
<br>@Temperature 23.0 °C
1.12 ft-lb/in
<br>@Temperature 73.4 °F
ISO 180/A
Cossa Polimeri ESTABLEND PA 6000 ABS / Nylon 6 Blend
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri..
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM 3.2mm
Asahi Kasei Xyron® NC42Z Modified Polyphenylene Ether
Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P..
Izod Impact, Notched 0.600 - 0.700 J/cm
1.12 - 1.31 ft-lb/in
IS 13411-1992
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color..
Izod Impact, Notched 0.600 - 0.700 J/cm
<br>@Temperature -30.0 - 0.000 °C
1.12 - 1.31 ft-lb/in
<br>@Temperature -22.0 - 32.0 °F
Average value: 0.692 J/cm Grade Count:1
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Izod Impact, Notched 0.600 - 0.800 J/cm
<br>@Temperature 0.000 - 0.000 °C
1.12 - 1.50 ft-lb/in
<br>@Temperature 32.0 - 32.0 °F
Average value: 0.468 J/cm Grade Count:4
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.600 J/cm
<br>@Temperature 23.0 °C
1.12 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram RamTal PM1027 Acetal, General Purpose
General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind.
Copyright © lookpolymers.com All Rights Reserved