Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.700 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.374 J/cm
<br>@Temperature 23.0 °C
0.700 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
RheTech Products G10P100-00 10% Glass Fiber Reinforced Polypropylene, Natural
Applications: BracketsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.374 J/cm
<br>@Temperature 23.0 °C
0.700 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
RheTech Products G10P100-01UV 10% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black
Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.374 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 22.8 °C
0.700 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.0 °F
injection molded ASTM Type 1 specimen; ASTM D256
Pinnacle Polymers 1112 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Izod Impact, Notched 0.374 J/cm
<br>@Temperature 23.0 °C
0.700 ft-lb/in
<br>@Temperature 73.4 °F
Method A; ASTM D256
Phillips 66 COPYLENE® CH043EW Polypropylene, Homopolymer, Slit Film, LWCO, Cordage
COPYLENE™ CH043EW is a medium flow polypropylene homopolymer resin suitable for general injection molding or extrusion applications. Applications: Raffia/tapes/strapping. Equivalent to Pro-fax® HL..
Izod Impact, Notched 0.374 J/cm
<br>@Temperature 23.0 °C
0.700 ft-lb/in
<br>@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Ineos H02C-00 Polypropylene Homopolymer
This is a low flow rate, high clarity homopolymer designed for extrusion, thermoforming, blow molding, and rigid packaging. Applications that require good see-through clarity combined with good hea..
Izod Impact, Notched 0.374 J/cm
<br>@Thickness 3.17 mm
0.700 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® ABS 04001 BK 10% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I..
Izod Impact, Notched 0.374 J/cm
<br>@Thickness 3.17 mm
0.700 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 0390 BK
Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.374 J/cm
<br>@Thickness 3.17 mm
0.700 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 0137 S2 Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.374 J/cm
<br>@Thickness 3.17 mm
0.700 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 0445 A
Availability: North AmericaForms: PelletsFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® N100MD2 (DAM) Nylon 6 with 2% MoS2 Lubricated
Information provided by Chase Plastics.
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® N300L (DAM) Nylon 6 (Utility Grade), Internally Lubricant
Information provided by Chase Plastics.
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Ensinger Tecatron® XP-64B Compression Molded PPS Compound, 40% Fiberglass, Black Pigmented
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Izod Impact, Notched 0.374 J/cm
<br>@Temperature 22.8 °C
0.700 ft-lb/in
<br>@Temperature 73.0 °F
ASTM D256
Clariant Renol PBT1100TF10 Polybutylene Terephthalate, PTFE Lubricated
Data provided by Clariant Masterbatches
Izod Impact, Notched 0.374 J/cm
<br>@Temperature 22.8 °C
0.700 ft-lb/in
<br>@Temperature 73.0 °F
ASTM D256
Clariant Renol PPSP0005 Polypropylene Homopolymer, Glass Fiber and Mica Reinforced, Chemically Coupled
Data provided by Clariant Masterbatches
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Aaron Industries AAROPRENE® TFPP 2010 Talc Filled Polypropylene
AAROPRENE® TFPP 2000 Series Talc Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256A
Braskem D180A2 Homopolymer Polypropylene
Description: Excellent Melt StabilityApplications: Suggested Uses Include Caps and Closures, Housewares, BCF Multi-Filaments, High Tenacity Continuous Filament Yarn, Fine Denier Staple FibersThis re..
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
Type &quot;A&quot;; ASTM D256
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide
Izod Impact, Notched 0.374 J/cm
<br>@Temperature 23.0 °C
0.700 ft-lb/in
<br>@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Ineos H07B-00 Polypropylene Homopolymer
This is a polypropylene homopolymer for cast film applications that require antiblock additives. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 17..
Izod Impact, Notched 0.374 J/cm
<br>@Temperature 23.0 °C
0.700 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.374 J/cm
<br>@Thickness 3.17 mm
0.700 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PBT FR-S
Availability: North AmericaForms: PelletsFeatures: Flame Retardant and Non-BloomingProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Copyright © lookpolymers.com All Rights Reserved