| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | DIN 53453; ASTM D256 |
| Kolon KOPA® KN111 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.38 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | DIN 53453; ASTM D256 |
| Kolon KOPET® KP132G30VO FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.38 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.38 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.38 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical Lupox® LW5402A PBT+PC+GF40% Description: Injection Molding, PBT+PC+GF40%, Low Warpage, High GlossApplication: E&E, Automotive (Bobbin, Switch)CAS No. 9010-86-0, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.38 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical Lupox® SG5300 PBT+PET+GF30% Description: Injection Molding, PBT+PET+GF30%, Good Surface Application: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | DIN 53453; ASTM D256 |
| Kolon KOPA® KN133G15 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | DIN 53453; ASTM D256 |
| Kolon KOPA® KN171 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | |
| Shinil Chemical SHINFLAME PA-6 GF Flame Retardant Polymer Parts SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.17 mm |
1.38 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® VB-5300G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.17 mm |
1.38 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Starex® BF-0670T MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.17 mm |
1.38 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Starex® BF-0670T MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.17 mm |
1.38 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.17 mm |
1.38 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | ASTM D256 |
| Cheng Yu Plastic NG1100S Nylon 66, 10% Glass Fiber Reinforced |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | ASTM D256 |
| Cheng Yu Plastic SW10 POM/PTFE |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | ASTM D256 |
| Cheng Yu Plastic FR200GV10 Flame Retardant Nylon 66, 10% Glass Fiber |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | ASTM D256 |
| Cheng Yu Plastic FR200N Flame Retardant Nylon 66 |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | ASTM D256 |
| Cheng Yu Plastic FV3030 Polyformaldehyde |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | ASTM D256 |
| Cheng Yu Plastic FV3035 Polyformaldehyde |
|||
| Izod Impact, Notched | 0.735 J/cm @Thickness 3.17 mm |
1.38 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Samsung Cheil Industries Infino® VB-5300G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | ASTM D256 |