Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.747 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Network Polymers NPP 25-3502
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.747 J/cm

@Temperature 23.0 °C
1.40 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Oxford Polymers 901-BK Polycarbonate/Polyetherimide Alloy
Polycarbonate/Polyetherimide AlloyInformation provided by Oxford Polymers.
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2..
Izod Impact, Notched 0.747 J/cm

@Diameter 3.17 mm,
Temperature 4.00 °C
1.40 ft-lb/in

@Diameter 0.125 in,
Temperature 39.2 °F
bar; ASTM D256
Ineos R01C-00 Polypropylene Random Copolymer
Grade R01C-00 is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding, through it is clarifier/antistat additive combination. Applications that requi..
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PA6 GF33 FR HS L BK065 33% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu..
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® ABS GF60 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.747 J/cm

@Temperature 22.8 °C
1.40 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302..
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® A220G ABS Molding Resin, 20% Glass Fiber Reinforced
Information provided by Chase Plastics.
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer
DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman.
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative
A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machinin..
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
0°F; ASTM D256A
Dow TF0807 TPO
Dow Fascia TPO for Painted ApplicationsInformation provided by Dow
Izod Impact, Notched >= 0.747 J/cm
>= 1.40 ft-lb/in
ASTM D256
Buckeye Polymers BP PPC 0235 BLK Polypropylene Copolymer
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis..
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
compression molded; ASTM D256
Americas Styrenics STYRON® 404 High Impact Polystyrene
Product CharacteristicsAdditive FreeTypical ApplicationsCompounding and masterbatchesInformation provided by AmericasStyrenics LLC.
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Copolymer CP0436G10CL Glass Reinforced
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Statiblend® PPS GF35 SS7 BK 35/7% Glass/Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel Fiber, 35/7% Filler by WeightUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Formosa Plastics Formolene® LH5204 Injection Molding HDPE  (discontinued **)
CopolymerApplications: Pails, lids and over-capsFormolene LH5204 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as ..
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Aaron Industries AAROPRENE® GFABS 4010 Glass Filled Acrylonitrile-Butadiene Styrene
AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PBT GF30 FR X 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantUL File Number: E157318TPCI# 1006011Information provided by TP Composites, In..