Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.854 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Network Polymers NPP 25-1902
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.854 J/cm

@Temperature 23.0 °C
1.60 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Oxford Polymers 20GF 20% Glass Fiber Reinforced ABS, Flame Retardant
20% Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers.
Izod Impact, Notched 0.854 J/cm

@Thickness 3.18 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Thermocomp® LF-1004 Polyetheretherketone, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Multibase Multi-Flamâ„¢ 0206 PP Polypropylene
Features:Flame RetardantHalogen Content, Low to None Forms:PelletsUses:TubingWire JacketingFurnitureInformation provided by Multibase
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA12 CM40 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 G/CF30 L BK 30% GlassCarbon Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: GlassCarbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedApp..
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 GF33 SL5 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Silicone Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized..
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PPA GF30 HS L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat..
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PPS F GF/M55 BK 55% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Teknor Apex Synres® PP G15 18 Polypropylene, Glass Reinforced
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many ..
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
0.125 in; ASTM D256
Chase Plastics CP Pryme® N120L (Dry) Nylon 6, 20% Glass Fiber Reinforced, Lubricated
Features: LubricatedForm: PelletsInformation provided by Chase Plastics.
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
0.125 in; ASTM D256
Chase Plastics CP Pryme® NN130M2 (Dry) Nylon 66, 30% Glass Fiber Reinforced, Lubricated
Features: Good chemical resistanceGood compressive strengthGood creep resistanceFast cycleLubricatedHigh rigiditySolvent resistanceHigh strengthForm: PelletsInformation provided by Chase Plastics.
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy
Information provided by A. Schulman.
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Aclo Accutech Polycarbonate POL051G10L Glass Reinforced
Izod Impact, Notched >= 0.854 J/cm
>= 1.60 ft-lb/in
ASTM D256
Buckeye Polymers BP PPC 0220 BLK Polypropylene Copolymer
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis..
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Asahi Kasei Thermylene® P6-30FG-0602 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
compression molded; ASTM D256
Americas Styrenics STYRON A-TECH® 1400AS High Impact Polystyrene
Product CharacteristicsHigh FlowGood ImpactFood Contact CompliantTypical ApplicationsTelevision housingsPrinter HousingsConsumer goodsInformation provided by AmericasStyrenics LLC.
Izod Impact, Notched 0.854 J/cm

@Thickness 3.18 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Polymer Resources PPX-FRG10 Modified PPO, UL 94 V-1, 10% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Izod Impact, Notched 0.854 J/cm

@Thickness 3.18 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Lubricomp® PDX-O-88533 BK8-229 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant  (disconti