Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.900 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific)
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
Izod Impact, Notched 0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Izod Impact, Notched 0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® LUX9130T PC COPOLYMER (Asia Pacific)
LUX9130T Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm / 5VA rating at 6.0mm and is U..
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone  (discontinued **)
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N..
Izod Impact, Notched 0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Asia Pacific)
Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. ..
Izod Impact, Notched 0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Izod Impact, Notched 0.900 J/cm

@Temperature 23.0 °C
1.69 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Lavergne VYPET VNT 645 PET 45% Glass Reinforced
Vypet VNT 645 is a 45% glass reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Excellent strength and stiffness; E..
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX5558 PPE+PS
30% glass reinforced, high flow PPO.
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Asia Pacific)
LNP* Lubricomp* MFL36S is a compound based on Polypropylene resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
Izod Impact, Notched 0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics ULTEM HU2300 PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON DEL32P PC (Asia Pacific)
LNP* Stat-kon* DEL32P is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive.
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
Light & White Colors; ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific)
Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade.
Izod Impact, Notched 0.900 J/cm

@Temperature 23.0 °C
1.69 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer
LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP UF0069S PPA
LNP THERMOCOMP* UF0069S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Izod Impact, Notched 0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® K3501 PBT (Europe-Africa-Middle East)
Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde..
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific)
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific)
LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding.
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC
LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Flame Retardant.
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOTUF VF003 PA 66
LNP* THERMOTUF* VF003 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Izod Impact, Notched 0.900 J/cm

@Temperature 23.0 °C
1.69 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamTal PM8427 Acetal, Impact modified
Impact modified polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 0.900 J/cm

@Thickness 3.17 mm
1.69 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers NPP30-0500 GF20 20% Glass Filled Black Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 0.900 J/cm

@Diameter 3.17 mm
1.69 ft-lb/in

@Diameter 0.125 in
bar, 0.010" notch radius; ASTM D256
Ineos Nova 5620 High Impact Polystyrene  (discontinued **)
High heat resistance, Good balance of toughness and rigidityApplications: Food service itemProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.I..
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific)
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated.
Copyright © lookpolymers.com All Rights Reserved