Polymer Property : Izod Impact, Notched = 0.900 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
73°F; ASTM D256
Multibase Multi-Pro® 5014 CUW Polypropylene
Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase
Izod Impact, Notched 0.481 J/cm
<br>@Thickness 6.35 mm
0.900 ft-lb/in
<br>@Thickness 0.250 in
ASTM D-256
Plaskolite Optix® CP - 927 High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Omni Plastics OmniLon™ 6/6 PA6/6 MF40 Mineral Filled Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
0.125 inch bar; ASTM D256
Network Polymers MS 175 Styrene Methyl Methacrylate Terpolymer
Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Ravago Manufacturing Americas Enviramid™ N2300HL BK/UV2 Post Consumer Recycle Nylon 6
Heat Stabilized, Lubricated, UV Stabilized, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Ravago Manufacturing Americas Hylon® N1020MHL Nylon 6/6 &nbsp;(discontinued **)
Available in North America Filler: Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedForm: Pellets Processing Method: Injection MoldingIn..
Izod Impact, Notched 0.481 - 2.67 J/cm
0.900 - 5.00 ft-lb/in
Average value: 1.10 J/cm Grade Count:15
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched 0.481 J/cm
<br>@Thickness 3.17 mm
0.900 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6/6 0146 A Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.481 J/cm
<br>@Thickness 3.17 mm
0.900 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PA6 TL10 Nylon 6
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (10%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Techmer ES Plaslube® AC-80/TF/20 BK1941 Acetal (POM) Copolymer
Izod Impact, Notched 0.481 J/cm
<br>@Thickness 3.17 mm
0.900 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PA6 FR HS
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT
Information provided by A. Schulman.
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6
Information provided by A. Schulman.
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT
Information provided by A. Schulman.
Izod Impact, Notched 0.481 J/cm
<br>@Temperature 22.8 °C
0.900 ft-lb/in
<br>@Temperature 73.0 °F
ASTM D256
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black
Data provided by Clariant Masterbatches
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336G10M20CL Glass/Mineral Reinforced Coupled
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256A
Braskem TR3350C Random Copolymer Polypropylene
Description: High melt flow, excellent see-through clarity, superior color and processing stability, low odor.Applications: Suggested uses include reusable food containers, housewares, fast-cycle in..
Izod Impact, Notched 0.481 J/cm
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
0.900 ft-lb/in
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Stat-Tech™ PI-05CF/000 EM Polyetherimide (PEI) &nbsp;(discontinued **)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D 256
Shakespeare Isocor™ HW29TL Nylon 610
Isocor™ HW29TL is an ultra low viscosity PA-610 with excellent melt flow characteristics. Isocor™ HW29TL is specifically formulated for thin wall or high speed injection molding applications. ..