Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 1.10 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.10 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne LubriOne™ SF-30GF/15T Polyphenylene Sulfide (PPS)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Izod Impact, Notched 1.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ GF 604 35 HS Black 13 Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
Izod Impact, Notched 1.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® PK-30GF/000 Polyetheretherketone (PEEK)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Izod Impact, Notched 1.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ 81520 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 1.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
PolyOne Geon™ Vinyl Dry Blend E7506 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon E7506 is recommended for whites and light pastel colors only. Performs well in extrusion blow molding and high rate fencing capstock applications.Physical properties based on Geon E7506 white 1..
Izod Impact, Notched 1.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Gravi-Tech™ GRV-NP-110-W-NAT Polyamide 12 (Nylon 12)
Information provided by PolyOne
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
SABIC PS 330 High Impact Polystyrene for Sheet Extrusion
Product Description: High Impact Polystyrene PS 330 is manufactured by continuous mass polymerization of styrene monomer. An elastomer is incorporated during polymerization to achieve impact resis..
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022..
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)  (discontinued **)
Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis..
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX4605 PPE+PS
PPE+PS blend. 20% Glass reinforced. High heat. Dimensional stability. Suitable for automotive and E/E applications.
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ISO 180
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Toyobo T-422-02R Nylon, Mineral-Reinforced
Key Feature: High heat distortion and good toughness, high flowInformation provided by Toyobo Co., Ltd
Izod Impact, Notched 1.10 J/cm

@Temperature 23.0 °C
2.06 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamTough PZ300G3 Polycarbonate, 15% Glass Fiber
15% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.10 J/cm

@Temperature 23.0 °C
2.06 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTACARB 0820 GF V0 HF Flame Retardant Polycarbonate
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good processability, good light resistanceI..
Izod Impact, Notched 1.10 J/cm

@Thickness 3.20 mm
2.06 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Makrolon® 9415(Z) Polycarbonate
Medium viscosity, flame retardant extrusion and injection molding grade with 10% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer Materia..
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
E-Polymers TEKANATE™ G730FR , Flame Retardant, 30% Glass Fiber Reinforced Poly Carbonate
30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Adell AR-37 Nylon 66, 35% Glass Reinforced
Data provided by Adell Plastics, Inc.
Izod Impact, Notched 1.10 J/cm

@Thickness 3.17 mm
2.06 ft-lb/in

@Thickness 0.125 in
ASTM Test
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d..
Izod Impact, Notched 1.10 J/cm

@Temperature -40.0 °C
2.06 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Ashley Polymers Ashlene® D925 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl..
Izod Impact, Notched 1.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne LubriOne™ PC-30GF/15T Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Izod Impact, Notched 1.10 J/cm

@Thickness 3.17 mm
2.06 ft-lb/in

@Thickness 0.125 in
ASTM D256
Covestro Apec® DP9-9353 High-Heat Polycarbonate, UV Stabilized  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Izod Impact, Notched 1.10 J/cm

@Thickness 3.17 mm
2.06 ft-lb/in

@Thickness 0.125 in
ASTM D256
Ascend Performance Materials VYDYNE® R533 Nylon, 33% Glass Reinforced
Typical property data. VYDYNE is a registered trademark of Solutia Inc.
Izod Impact, Notched 1.10 J/cm

@Temperature -30.0 °C
2.06 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256A
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer
Key Features: fast crystallization shortens cycle times, excellent cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: automotive blow molded partsMeets FDA requir..
Copyright © lookpolymers.com All Rights Reserved