| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
0.587
J/cm <br>@Temperature 23.0 °C
|
1.10
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
Oxford Polymers 15GF-V0 15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), Flame Resistant
15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), Flame ResistantInformation provided by Oxford Polymers.
|
|||
| Izod Impact, Notched |
0.587
J/cm <br>@Temperature 23.0 °C
|
1.10
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
Oxford Polymers 30CF 30% Carbon Fiber Reinforced Polyphenylene Sulfide
30% Carbon Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers.
|
|||
| Izod Impact, Notched |
0.587
J/cm <br>@Thickness 3.17 mm
|
1.10
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced
Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor..
|
|||
| Izod Impact, Notched | 0.588 - 1.60 J/cm | 1.10 - 3.00 ft-lb/in | Average value: 0.956 J/cm Grade Count:16 |
|
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
|
|||
| Izod Impact, Notched |
0.588
J/cm <br>@Thickness 6.40 mm,<br> Temperature 23.0 °C
|
1.10
ft-lb/in <br>@Thickness 0.252 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Izod Impact, Notched |
0.588
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
1.10
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant
Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
|
|||
| Izod Impact, Notched |
0.587
J/cm <br>@Thickness 3.17 mm
|
1.10
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES Electrafil® DB-1200/S/7/FR ABS, 7% Stainless Steel Fiber Reinforced (dry blend), Flame Retardant
Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL..
|
|||
| Izod Impact, Notched |
0.587
J/cm <br>@Thickness 3.17 mm
|
1.10
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES HiFill® PA6 GF13 L BK 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp..
|
|||
| Izod Impact, Notched |
0.587
J/cm <br>@Thickness 3.17 mm
|
1.10
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES HiFill® PA6/6 GF13 TL10 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: PTFE Lubricant (10%)Features: LubricatedAppearance: Natural ColorInformation ..
|
|||
| Izod Impact, Notched |
0.587
J/cm <br>@Thickness 3.17 mm
|
1.10
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES HiFill® POM CO 0150 S Acetal
Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: CopolymerInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
0.587
J/cm <br>@Thickness 3.17 mm
|
1.10
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES Luriblend® PEI GF30 TL15 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | 0.125 in; ASTM D256 |
|
Chase Plastics CP Pryme® N320L (Dry) Nylon 6, 20% Glass Fiber Reinforced, Lubricated, Recycled Content
Features: LubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics.
|
|||
| Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
|
Chase Plastics CP Pryme® NN100HSL (DAM) Nylon 66, Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
|
Aclo Accutech Polypropylene Homopolymer HP0334G25M5CL Glass/Mineral Reinforced Coupled |
|||
| Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
|
Asahi Kasei Thermylene® P6-20FG-2153R 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Izod Impact, Notched | 0.587 - 0.801 J/cm | 1.10 - 1.50 ft-lb/in | ASTM D256 |
|
Aaron Industries AVPS M 100-2 Virgin Polystyrene
Melt flow index may be specified.
|
|||
| Izod Impact, Notched | 0.587 J/cm | 1.10 ft-lb/in | ASTM D256 |
|
Aaron Industries AAROPRENE® GFN 6013 Glass Filled Nylon 6
AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified.
|
|||
| Izod Impact, Notched | 0.587 - 10.7 J/cm | 1.10 - 20.0 ft-lb/in | Average value: 2.31 J/cm Grade Count:11 |
|
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and ..
|
|||
| Izod Impact, Notched |
0.587
J/cm <br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
|
1.10
ft-lb/in <br>@Thickness 0.250 in,<br> Temperature 73.4 °F
|
Method A, Injection Molded; ASTM D256 |
|
PolyOne Stat-Tech™ AS-30GF/000 SD Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedAntistaticInformation provided by PolyOne Corporation.
|
|||
| Izod Impact, Notched | 0.587 - 1.60 J/cm | 1.10 - 3.00 ft-lb/in | Average value: 0.891 J/cm Grade Count:25 |
|
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
|
|||
| Izod Impact, Notched |
0.587
J/cm <br>@Temperature 23.0 °C
|
1.10
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
RheTech Products G20P100-406 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUEA) Midnight Black
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||