Mechanical Properties Metric English Comments
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
NYCOA 27/330KNF Glass Filled Nylon 6
33% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc.
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Omni Plastics OmniLon™ 6/6 PA6/6 GR15 IM10 Glass Reinforced/Impact Modified Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Izod Impact, Notched 1.23 J/cm

@Temperature 22.8 °C
2.30 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources NY66-G43 Nylon 66, 43% Glass Reinforced
Nylon 66, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
Izod Impact, Notched 1.23 J/cm

@Temperature 22.8 °C
2.30 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized
Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Izod Impact, Notched 1.23 J/cm

@Temperature -30.0 °C
2.30 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
73°F; ASTM D256
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (Cond) &nbsp;(discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256-A
Ineos Styrenics 495F High-Impact Polystyrene Resin (Global)
Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa..
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256-A
Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global)
Description: Avantra® 2710 is a high-impact grade of polystyrene with improved stress crack resistance, developed primarily for extrusion and thermoforming applications, especially for the refrig..
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256-A
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene
Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applic..
Izod Impact, Notched 1.23 J/cm

@Thickness 3.20 mm
2.30 ft-lb/in

@Thickness 0.126 in
ASTM D256
KKPC Kuhmo HFH 403 Flame Retarded HIPS
Key features: Low flammable V-2 grade. Common Uses: TV and VCR housing.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resis..
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm
2.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PA6/6 FR HS BK (Conditioned)
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Stratasys® PC-ABS
PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior mechanical properties and heat resis..
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm
2.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Plastiblend® PA6 GF20 RM L BK Nylon 6
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Low Moisture Absorption and LubricatedBlackTPCI# 9718102Inf..
Izod Impact, Notched 1.23 J/cm

@Thickness 6.35 mm
2.30 ft-lb/in

@Thickness 0.250 in
ASTM D256
PlastxWorld CEVIAN® CGF10 10% GF PC/Acrylic Alloy
Glass fiber reinforced PC/Acrylic alloy.These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc.
Izod Impact, Notched 1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
Method B; Brittle/Ductile Failure
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6
26% crystallinity. Information supplied by Elastomer Engineering.
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Washington Penn Medium Impact Copolymer 10% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Izod Impact, Notched 1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite Butyrate 565A3720023 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Izod Impact, Notched 1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite Propionate 384A4000016 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Diamond Polymers TR 5000 AS/P
Description: Transparent ABS, Antistatic GradeInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Cheng Yu Plastic A703G25 ABS 25% Glass Fiber Reinforced
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 520-40G Nylon 66, 40% Glass Reinforced
A general purpose 40% glass reinforced Nylon 66 resin.Data provided by the manufacturer
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256-93a
Multibase Multi-ABS 3525 Black
Moisture content is 0.08%.Data provided by Multibase.
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman.
Izod Impact, Notched 1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Ashley Polymers Ashlene® P270 PPO
An extrusion grade for high temperature applications as well as high mechanical strength and toughness such as electrical housings.Data provided by the manufacturer
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
0.125 in.; ASTM D256
Resirene Resirene® 6110 High Impact Polystyrene
Features:High ImpactEasy ProcessingFDA Rating: 21 CFR 177.1640FlexibilityApplications:Injection MoldingTV CabinetsRemote ControlsToysInformation provided by US distributor Calsak Corporation.
Izod Impact, Notched 1.23 J/cm

@Temperature 23.0 °C
2.30 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.