| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
PolyOne Stat-Tech™ NN-40CF/000 FRV0 Natural Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Izod Impact, Notched |
0.680
J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.27
ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
|
Polimeri Europa Edistir R 321P Polystyrene
Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30Applic..
|
|||
| Izod Impact, Notched |
0.680
J/cm @Temperature -30.0 °C |
1.27
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
PolyOne Edgetek® NN-40CF/000 FRV0 NATURAL Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
Plenco 51240 PET, Pellet, Injection Molded, Black
(discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
|
|||
| Izod Impact, Notched |
0.680
J/cm @Temperature 23.0 °C |
1.27
ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
|
LATI LATILUB 73/13-20ST Polyoxymethylene Base (POM), 20% Mixed PTFE/Silicone Self Lubricating Plastic
(discon
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
|
|||
| Izod Impact, Notched | >= 0.680 J/cm | >= 1.27 ft-lb/in | Method A; ASTM D 256 |
|
Karina 806-18/364-BY-ERYB Gray PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal
LNP LUBRILOY* KL201 is a compound based on Acetal resin containing Proprietary Lubricant. PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Asia Pacific)
LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East)
LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON DD0009 PC
LNP* STAT-KON* DD0009 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Asia Pacific)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Izod Impact, Notched |
0.680
J/cm @Temperature 23.0 °C |
1.27
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT
LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP OF008G PPS - LINEAR
LNP* THERMOCOMP* OF008G is a compound based on PPS - Linear containing 15% Glass Fiber, 25% Milled Glass.
|
|||
| Izod Impact, Notched |
0.680
J/cm @Temperature -30.0 °C |
1.27
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
|
|||
| Izod Impact, Notched |
0.680
J/cm @Temperature -30.0 °C |
1.27
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
|
|||
| Izod Impact, Notched |
0.680
J/cm @Temperature -30.0 °C |
1.27
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East)
Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s..
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL HM4025H PPE+PS (Asia Pacific)
40% GF/MF filled FR PPE/PS blend, high flow
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL NF2020 PPE+PS (Asia Pacific) |
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL PCN2910 PPE+PS (Asia Pacific)
35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C
LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI
LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL CN1134 PPE+PS (Asia Pacific)
20% filled FR high modulus PPE/PS blend
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL CN5258 PPE+PS (Asia Pacific)
40% filled FR high modulus PPE/PS blend
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, 50% RH
Neat resin, for injection molding.Information provided by Cresset Powers Ltd.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET
40% GF/MF Reinforced, Low warpageInformation provided by E-Polymers Co. Ltd.
|
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL CN5246 PPE+PS (Asia Pacific) |
|||
| Izod Impact, Notched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D256 |
|
Plenco 50130 PET, Pellet, Injection Molded, Black
(discontinued **)
PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat..
|
|||