Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 1.30 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.30 J/cm
<br>@Thickness 3.18 mm,<br> Temperature 23.0 °C
2.44 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne LubriOne™ PC-000/20T Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Nylene® PA6/6 Glass Filled 5143 HS Nylon 6/6
43% Glass Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Izod Impact, Notched 1.30 J/cm
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
2.44 ft-lb/in
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® PC-20GF/000 Polycarbonate (PC)
Information provided by PolyOne
Izod Impact, Notched 1.30 J/cm
<br>@Thickness 3.18 mm,<br> Temperature 23.0 °C
2.44 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
ASTM D256
PolyOne Geon™ CPVC MC550 Polyvinyl Chloride, Chlorinated (CPVC)
Information provided by PolyOne
Izod Impact, Notched 1.30 J/cm
<br>@Temperature -30.0 °C
2.44 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific)
Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame..
Izod Impact, Notched 1.30 J/cm
<br>@Thickness 3.18 mm,<br> Temperature 23.0 °C
2.44 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ ND633 GF Natural Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
Izod Impact, Notched 1.30 J/cm
<br>@Temperature -30.0 °C
2.44 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Izod Impact, Notched 1.30 J/cm
<br>@Thickness 3.17 mm
2.44 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Fiberfil® FV-30 Nylon 6, 30% Glass Reinforced, Heat Stabilized
Information provided by FIBERFIL Engineered Plastics
Izod Impact, Notched 1.30 J/cm
<br>@Thickness 3.17 mm
2.44 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Fiberfil® FV-31 Nylon 6, 31% Glass Reinforced, Heat Stabilized
Information provided by FIBERFIL Engineered Plastics
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
23° C; ASTM D256
Flint Hills AP6106-HS Impact Copolymer Polypropylene
High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: child protection systems, appliance components, consumer durables, and automotive in..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
23° C; ASTM D256
Flint Hills AP6120-HS Impact Copolymer Polypropylene
High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
23° C; ASTM D256
Flint Hills AP6412-HS Impact Copolymer Polypropylene
High impact copolymer, and FDA compliant. Features: Blush resistant and heat stabilized.Applications: Injection molding: consumer durables, automotive interior trim, furniture trim and housing, and ..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256A
LyondellBasell Astryn BA35H Polypropylene Copolymer, Flame Retardant
Key Features: conventional melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colora..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
73°F; ASTM D256
LyondellBasell Hifaxâ„¢ EP2015/60 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ EP2015/60 medium melt flow, 690 MPa flexural modulus, extrusion coating grade, specialty polypropylene copolymer has a very good balance of properties and processability. Th..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry)
Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON MX10301C PP
LNP* STAT-KON* MX10301C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Izod Impact, Notched 1.30 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
2.44 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.4 °F
0.25 mm Notch Depth; ASTM D256
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi..
Izod Impact, Notched 1.30 J/cm
<br>@Thickness 3.20 mm
2.44 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Supreme Petrochem SP 6450 High Heat Polystyrene
Characteristics High impact and modulus Very good flow properties High heat resistance & strength Available in any dark colorProcessing Injection moldingApplications Instrument enclosures Automo..
Izod Impact, Notched 1.30 J/cm
<br>@Temperature 23.0 °C
2.44 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram PlusTek PA303G33 Nylon 6.6, 33% Glass Fiber
33% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.30 J/cm
<br>@Temperature 23.0 °C
2.44 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram PlusTek PA303G50 Nylon 6.6, 50% Glass Fiber
50% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ISO 180
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ISO 180
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Izod Impact, Notched 1.30 J/cm
<br>@Temperature 23.0 °C
2.44 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Polyram RamTough RZ310G6 Polycarbonate, 30% Glass Fiber
30% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric stren..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced
Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced
Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
E-Polymers TEKAMID® TA250G33 33% Glass Fiber Reinforced PA66, DAM
33% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 1410B Polycarbonate, 8-10% Glass Reinforced
A rigid black polycarbonate, for applications requiring superior dimensional stability and overall toughness. Contains 8-10% glass reinforcement. Also available: 1413B, UV stabilized.Data provided..
Izod Impact, Notched 1.30 - 1.30 J/cm
<br>@Temperature -40.0 - -40.0 °C
2.44 - 2.44 ft-lb/in
<br>@Temperature -40.0 - -40.0 °F
Average value: 1.30 J/cm Grade Count:2
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D265
Solvay TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY
Description: Polyamide 6, 30% glass fiber reinforced, for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 1021GF6 is used in all sectors of industry, offering an excelle..
Copyright © lookpolymers.com All Rights Reserved