| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.380 - 0.700 J/cm | 0.712 - 1.31 ft-lb/in | Average value: 0.565 J/cm Grade Count:4 |
|
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep..
|
|||
| Izod Impact, Notched |
0.280
-
0.700
J/cm <br>@Temperature -40.0 - -20.0 °C
|
0.525
-
1.31
ft-lb/in <br>@Temperature -40.0 - -4.00 °F
|
Average value: 0.321 J/cm Grade Count:4 |
|
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
|
|||
| Izod Impact, Notched | 0.500 - 0.700 J/cm | 0.937 - 1.31 ft-lb/in | ASTM D256 |
|
Loxim 821 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant
Information provided by Loxim Industries
|
|||
| Izod Impact, Notched | 0.500 - 0.700 J/cm | 0.937 - 1.31 ft-lb/in | ASTM D256 |
|
Shuman 811 Black Polystyrene Medium Impact
Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer.
|
|||
| Izod Impact, Notched | 0.500 - 0.700 J/cm | 0.937 - 1.31 ft-lb/in | ASTM D256 |
|
Shuman 881 Grey Polystyrene Medium Impact
Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer.
|
|||
| Izod Impact, Notched |
0.500
-
0.700
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
0.937
-
1.31
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256, ISO 180/4a |
|
EPICHEM PA 6 GF 30 Polyamide 6, 30% Glass
Characteristics: medium viscosity, 30% glass fibre filled
|
|||
| Izod Impact, Notched |
0.500
-
0.700
J/cm <br>@Thickness 6.35 mm
|
0.937
-
1.31
ft-lb/in <br>@Thickness 0.250 in
|
ASTM D256 |
|
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
|
|||
| Izod Impact, Notched |
0.500
-
0.700
J/cm <br>@Thickness 6.35 mm
|
0.937
-
1.31
ft-lb/in <br>@Thickness 0.250 in
|
ASTM D256 |
|
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
|
|||
| Izod Impact, Notched | 0.600 - 0.700 J/cm | 1.12 - 1.31 ft-lb/in | IS 13411-1992 |
|
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color..
|
|||
| Izod Impact, Notched |
0.500
-
0.700
J/cm <br>@Thickness 6.35 mm
|
0.937
-
1.31
ft-lb/in <br>@Thickness 0.250 in
|
ASTM D256 |
|
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
|
|||
| Izod Impact, Notched |
0.600
-
0.700
J/cm <br>@Temperature -30.0 - 0.000 °C
|
1.12
-
1.31
ft-lb/in <br>@Temperature -22.0 - 32.0 °F
|
Average value: 0.692 J/cm Grade Count:1 |
|
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
|
|||
| Izod Impact, Notched |
0.600
-
0.700
J/cm <br>@Thickness 3.20 - 3.20 mm
|
1.12
-
1.31
ft-lb/in <br>@Thickness 0.126 - 0.126 in
|
Average value: 0.692 J/cm Grade Count:1 |
|
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
|
|||