Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 1.40 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.747 J/cm

@Temperature 23.0 °C
1.40 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black
Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Nylene® 9533 , 33% Glass Reinforced Nylon 6/12
Description: Nylene® 9533 is a 33% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resou..
Izod Impact, Notched 0.747 J/cm

@Thickness 3.18 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
0.125 in, 73°F; ASTM D256
Matrixx Group 80S7301 30% Glass Reinforced PET  (discontinued **)
Data provided by The Matrixx Group, formerly RePlas.
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
M. Holland Company RP700 Polypropylene Copolymer
Features: Antistatic, Medium Clarity, Good FlowUses: Household Goods, KitchenwareApprovals: FDA 21 CFR 176.170(c), Table 2, Cond. B, C, D, E, F, G and HProcessing Method: Injection MoldingInformatio..
Izod Impact, Notched 0.747 J/cm

@Diameter 3.17 mm,
Temperature 4.00 °C
1.40 ft-lb/in

@Diameter 0.125 in,
Temperature 39.2 °F
bar; ASTM D256
Ineos R01C-00 Polypropylene Random Copolymer
Grade R01C-00 is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding, through it is clarifier/antistat additive combination. Applications that requi..
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Statiblend® PA6/6 02013
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedUL File Number: E157318TPCI# 1039101Informati..
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Aclo Accutech ABS ABS833G10L Glass Reinforced
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256A
Braskem TR3020F Random Copolymer Polypropylene
Description: High flexural modulus. Applications: Suggested uses include extrusion, blow molding. Process: Extrusion. This resin meets the requirements for olefin polymers as defined in 21 CFR, se..
Izod Impact, Notched >= 0.747 J/cm
>= 1.40 ft-lb/in
ASTM D256
Buckeye Polymers BP PPC 0235 BLK Polypropylene Copolymer
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis..
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Copolymer CP0436G10CL Glass Reinforced
Izod Impact, Notched 0.747 J/cm

@Temperature 23.0 °C
1.40 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Oxford Polymers 30GF-25PTFE 30% Glass Fiber/PTFE Reinforced Polyphenylene Sulfide  (discontinued **)
30% Glass Fiber/PTFE Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers.