| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature -30.0 °C
|
1.59
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER
Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and ..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature -30.0 °C
|
1.59
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature -30.0 °C
|
1.59
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Asia Pacific)
Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature -30.0 °C
|
1.59
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**)
Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with ..
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide Compound
(Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
1.59
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
Kingfa PA66-G15 15% Glass Fiber Reinforced PA66
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature 23.0 °C
|
1.59
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature 23.0 °C
|
1.59
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
Lavergne VYPET VNT 615 PET 15% Glass Reinforced
Vypet VNT 615 is a 15% fiberglass reinforced PET injection molding compound designed for structural applications.Features: Easy, fast processing; Excellent strength and stiffness; Excellent dimensio..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature 23.0 °C
|
1.59
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D 256 |
|
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific)
LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi..
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66 (Asia Pacific)
LNP* Lubricomp* RX05496 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics ULTEM 2300 PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics ULTEM 2300 PEI (Asia Pacific)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics ULTEM HU2300 PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature 0.000 °C
|
1.59
ft-lb/in <br>@Temperature 32.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON PE002Z PA 6
LNP* STAT-KON* PE002Z is a compound based on Nylon 6 resin containing 10% Carbon Fiber. Added features of this grade include: Extrusion Grade.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SPS Guang Zhou POBUXâ„¢ 3001EPG30 Non-halogen flame retardance/GF30%-PBT
Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) ..
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Asia Pacific)
LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP IF007 PA 6/12 (Asia Pacific)
LNP* THERMOCOMP* IF007 is a compound based on Nylon 6/12 resin containing Glass Fiber.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP KF006 Acetal Copoly
LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 (Asia Pacific)
LNP* Thermocomp* RFB66 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® HX420HP PBT
Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East)
Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS (Asia Pacific)
LNP* Thermocomp* AF004L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible.
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature 23.0 °C
|
1.59
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D 256 |
|
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK
LNP THERMOCOMP* LF004 is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA (Asia Pacific)
LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing Glass Fiber.
|
|||
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
|
A. Schulman ComAlloy Comtuf® 464 Glass Reinforced, Impact Modified, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature -30.0 °C
|
1.59
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Asia Pacific)
Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
|
|||
| Izod Impact, Notched |
0.850
J/cm <br>@Temperature 23.0 °C
|
1.59
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM-D256 |
|
Polyram RamTal PM3007G6 Acetal, 30% Glass Fiber
30% Glass-fiber reinforced polyacetal for injection molding applications.Information provided by Polyram Ram On Ind.
|
|||