| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
0.854
J/cm @Temperature 23.0 °C |
1.60
ft-lb/in @Temperature 73.4 °F |
Method A; ASTM D256 |
|
Phillips 66 COPYLENE® CM500LN Polypropylene, Impact Copolymer, High Flow, Medium Impact, Nucleated, Lube, Injection Molding
COPYLENE™ CM500LN is a very high melt flow, medium impact polypropylene copolymer resin, designed for injection molding applications requiring a good balance of properties with faster cycling capab..
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 3.18 mm |
1.60
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
LNP Lubricomp® OFL-4036 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.60
ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
|
PolyOne Lubri-Tech™ AS-20GF/05T Acrylonitrile Butadiene Styrene (ABS), Glass Filled, PTFE Lubricated
(discont
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Izod Impact, Notched | 0.854 J/cm | 1.60 ft-lb/in | ASTM D256 |
|
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC
(discontinued **)
Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:..
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 3.17 mm |
1.60
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 3.17 mm |
1.60
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Izod Impact, Notched |
0.854
J/cm @Temperature 22.8 °C |
1.60
ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
|
Spartech PP5440 Glass Fiber Reinforced Homopolymer
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 3.17 mm |
1.60
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Techmer ES HiFill® PA6 GF20 L UV 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 3.17 mm |
1.60
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Techmer ES HiFill® PA6 GF20 L UV BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 3.17 mm |
1.60
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Techmer ES HiFill® PEEK CF30 HF 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 3.17 mm |
1.60
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Techmer ES Electrablend® PA6 04001 BL Glass/Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated and Radio Frequency Shielding (RFI..
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 3.17 mm |
1.60
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b..
|
|||
| Izod Impact, Notched | 0.854 J/cm | 1.60 ft-lb/in | ASTM D256 |
|
A. Schulman COMTUF® 464 Glass Reinforced Impact Modified PBT Alloy
Information provided by A. Schulman.
|
|||
| Izod Impact, Notched |
0.854
J/cm @Temperature 22.8 °C |
1.60
ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
|
Clariant Renol PA113G13X050 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Improved Ductility
Data provided by Clariant Masterbatches
|
|||
| Izod Impact, Notched | 0.854 J/cm | 1.60 ft-lb/in | ASTM D256 |
|
Asahi Kasei Thermylene® P6-20FG-0753 20% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Izod Impact, Notched | 0.854 J/cm | 1.60 ft-lb/in | ASTM D256 |
|
Aclo Accutech Polypropylene Copolymer CP0436G5M25CL Glass/Mineral Reinforced Coupled |
|||
| Izod Impact, Notched | 0.854 J/cm | 1.60 ft-lb/in | ASTM D256 |
|
Aaron Industries AAROPRENE® GFIPP 2020 High Impact Glass Filled Polypropylene
AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
|
|||
| Izod Impact, Notched |
0.854
J/cm @Thickness 3.18 mm |
1.60
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Izod Impact, Notched | 0.854 J/cm | 1.60 ft-lb/in | ASTM D256 |
|
Polymer Resources PPX-FRG10 Modified PPO, UL 94 V-1, 10% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||