| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
0.880
J/cm @Temperature -30.0 °C |
1.65
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS
Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes..
|
|||
| Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
|
Reliance Industries Relene M60075 Polyethylene
Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade..
|
|||
| Izod Impact, Notched | 0.883 J/cm | 1.65 ft-lb/in | Notched/Unnotched not specified; ASTM D256A |
|
Total Lacqrene® 3351(AS) Impact Polystyrene
(discontinued **)
LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona..
|
|||
| Izod Impact, Notched | 0.883 J/cm | 1.65 ft-lb/in | ASTM D256 |
|
PTS Lucet® GC-225 25% Glass Reinforced Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.65
ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
|
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity
Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Izod Impact, Notched | 0.881 J/cm | 1.65 ft-lb/in | ASTM D256 |
|
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT
Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched |
0.880
J/cm @Temperature -20.0 °C |
1.65
ft-lb/in @Temperature -4.00 °F |
|
|
Kuraray SEPTON® CM2 Compatibilizer
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo..
|
|||
| Izod Impact, Notched |
>=
0.883
J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>=
1.65
ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
|
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow
Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica..
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.65
ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
|
LG Chemical Lupox® SG5500 PBT+PET+GF50%
Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.65
ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
|
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose
Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical
|
|||
| Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL S100G10 PPE+PS (Asia Pacific) |
|||
| Izod Impact, Notched | 0.883 J/cm | 1.65 ft-lb/in | |
|
Shinil Chemical SHINCON PEEK-CF LCD Rack
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b..
|
|||
| Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7602 PC (Asia Pacific) |
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.17 mm |
1.65
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Samsung Cheil Industries Starex® NH-1907 HIPS, Unreinforced FR
Information provided by Samsung Cheil Industries.
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.65
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
|
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
|
|||
| Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Asia Pacific)
PPE+PS blend. 20% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump..
|
|||
| Izod Impact, Notched |
0.880
J/cm @Temperature 23.0 °C |
1.65
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics Noryl GTX GTX880 PPE+PA6 (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.65
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
|
Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.65
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
|
Shinkong Synthetic Fibers Shinite® F102G30 PET, 30% Glass Filled, Fire Retardant, Halogen Free
Information from Shinkong Synthetic Fibers Corp.
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.17 mm |
1.65
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Samsung Cheil Industries Infino® VB-5400G PBT, Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.17 mm |
1.65
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced
PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries.
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.65
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
|
Shinkong Synthetic Fibers Shinite® D202G30 PBT, 30% Glass Filled, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
|
|||
| Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics NORYL GTX APS130 PPE+PPS (Asia Pacific)
PPE+PPS GF30%
|
|||
| Izod Impact, Notched | 0.883 - 1.87 J/cm | 1.65 - 3.50 ft-lb/in | Average value: 1.38 J/cm Grade Count:14 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
|
|||
| Izod Impact, Notched | 0.883 J/cm | 1.65 ft-lb/in | ASTM D256A |
|
Total Lacqrene® 814(AS) High Impact Polystyrene
(discontinued **)
LACQRENE® 814 is a high impact, flame retardant polystyrene, free from PBDPE and with excellent thermal stability.ApplicationCovers for electrical equipment, Office equipment: copiers, faxInformati..
|
|||
| Izod Impact, Notched |
>=
0.883
J/cm @Thickness 6.35 mm |
>=
1.65
ft-lb/in @Thickness 0.250 in |
ASTM D256 |
|
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||
| Izod Impact, Notched |
>=
0.883
J/cm @Thickness 6.35 mm |
>=
1.65
ft-lb/in @Thickness 0.250 in |
ASTM D256 |
|
Gromax CCP PET 9130-200 30% Glass Filled
Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell..
|
|||
| Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® LC108 PC (Asia Pacific)
Polycarbonate base, 8% carbon fiber reinforced, FR
|
|||
| Izod Impact, Notched |
0.883
J/cm @Thickness 3.17 mm |
1.65
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Samyang Trihip® B300 High Impact Polystyrene, Flame Retardant
Dimensional stability, electrical properties and weather resistance are excellent.B300 is the flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, Print..
|
|||