Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
73°F; ASTM D256
Multibase Nylex™ 2185 NAT Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Izod Impact, Notched 0.910 J/cm
<br>@Thickness 3.18 mm,<br> Temperature 23.0 °C
1.70 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ GF 1200 33 Red 31 A Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Network Polymers NPP 808 C5WW
Description: Polycarbonate AlloyInformation provided by Network Polymers Inc.
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Ravago Manufacturing Americas Hylon® N2233HL BK Nylon 6
Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces..
Izod Impact, Notched 0.908 J/cm
<br>@Thickness 3.20 mm,<br> Temperature 22.8 °C
1.70 ft-lb/in
<br>@Thickness 0.126 in,<br> Temperature 73.0 °F
injection molded ASTM Type 1 specimen; ASTM D256
Pinnacle Polymers 2150 H Medium Impact Polypropylene Copolymer, Injection Molding Grade
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Polymer Resources PPX-FRG20 Modified PPO, UL 94 V-1, 20% Glass Reinforced &nbsp;(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Izod Impact, Notched 0.908 J/cm
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
1.70 ft-lb/in
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Lubri-Tech™ PI-10CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated &nbsp;(discontinued
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.910 J/cm
<br>@Temperature -40.0 °C
1.70 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
Ineos ABS Centrex® 401 AES Extrusion &nbsp;(discontinued **)
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Izod Impact, Notched 0.907 J/cm
<br>@Thickness 3.18 mm
1.70 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
LNP Thermocomp® STN-F-1006 HS Polyamide 46, Glass Fiber Reinforcement &nbsp;(discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..
Izod Impact, Notched 0.908 J/cm
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
1.70 ft-lb/in
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® SF-47GF/000 Polyphenylene Sulfide (PPS), Glass Filled &nbsp;(discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
Kolon KOCETAL® LF302 Wear Modified Acetal Resin
Improved wear property and dimensional stability. Applications: Products for low noise and precision gear. Information provided by API-Kolon.
Izod Impact, Notched 0.908 J/cm
<br>@Thickness 3.17 mm
1.70 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 G/C50 A240 BK 50% Glass/Ceramic Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 50% Filler by WeightAppearance: BlackTPCI# 9809102Information provided by TP Composites, Inc.
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Styron EMERGEâ„¢ 4702-8 Polycarbonate
EMERGEâ„¢ PC 4702-8 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat resi..
Izod Impact, Notched 0.908 J/cm
<br>@Thickness 3.17 mm
1.70 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
PlastxWorld CEVIAN® LMW48 Laser Markable Grade ABS
White MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET
Information provided by A. Schulman.
Izod Impact, Notched 0.907 J/cm
<br>@Thickness 3.17 mm,<br> Temperature 23.0 °C
1.70 ft-lb/in
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
ASTM D256
Diamond Polymers NPP 808 C5 TDS Polycarbonate Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Aclo Accutech ABS ABS832G40L Glass Reinforced
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 262 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 0.908 J/cm
<br>@Temperature 23.0 °C
1.70 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D256
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene &nbsp;(discontinued **)
Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L..
Copyright © lookpolymers.com All Rights Reserved