| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
6.90
J/cm <br>@Thickness 3.18 mm,<br> Temperature 23.0 °C
|
12.9
ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F
|
Injection Molded; ASTM D256A |
|
PolyOne Trilliant™ HC HC3620-0040 RS Natural Polycarbonate + PBT (PC+PBT)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
|
|||
| Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer
Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.
|
|||
| Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific)
Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.
|
|||
| Izod Impact, Notched |
6.90
J/cm <br>@Temperature -10.0 °C
|
12.9
ft-lb/in <br>@Temperature 14.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Europe-Africa-Middle East)
19 MFR LEXAN High Flow Ductile Copolymer with 400 nm cut off, available in transparent colors only
|
|||
| Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
|
|||
| Izod Impact, Notched |
6.90
J/cm <br>@Thickness 3.17 mm
|
12.9
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Izod Impact, Notched |
6.86
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
12.9
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability
Feature: Injection Molding, PA6/ABS, High Impact, Good Dimensional StabilityApplication: Pipe Fitting, Electrical and Electronic partsCAS No. 25038-54-4, 9003-56-9 and 9003-54-7Information provided ..
|
|||
| Izod Impact, Notched |
6.86
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
12.9
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical Lupox® TE5011M PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG ..
|
|||
| Izod Impact, Notched |
>=
6.86
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
>=
12.9
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information ..
|
|||
| Izod Impact, Notched |
>=
6.86
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
>=
12.9
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical LUPOY SC5004T PC/Polyester, Transparency
Description: Injection Molding, PC/Polyester, General Purpose, Transparency, High FlowApplication: Keypad for Mobile PhoneCAS: 103598-77-2Information provided by LG Chemical
|
|||
| Izod Impact, Notched |
6.86
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
12.9
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical Lupox® TE5000GH PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Garnish)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical
|
|||
| Izod Impact, Notched |
>=
6.86
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
>=
12.9
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| Izod Impact, Notched |
>=
6.86
J/cm <br>@Thickness 3.20 mm,<br> Temperature 23.0 °C
|
>=
12.9
ft-lb/in <br>@Thickness 0.126 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
LG Chemical LUPOY GP1000LS PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided ..
|
|||
| Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled
Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h..
|
|||
| Izod Impact, Notched |
6.90
J/cm <br>@Thickness 3.18 mm
|
12.9
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
|
|||
| Izod Impact, Notched |
6.91
J/cm <br>@Temperature 0.000 °C
|
12.9
ft-lb/in <br>@Temperature 32.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Xenoy® 5720U PBT+PC
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
|
|||
| Izod Impact, Notched |
6.91
J/cm <br>@Temperature 0.000 °C
|
12.9
ft-lb/in <br>@Temperature 32.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
|
|||
| Izod Impact, Notched |
6.91
J/cm <br>@Temperature 0.000 °C
|
12.9
ft-lb/in <br>@Temperature 32.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
|
|||
| Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC
LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc..
|
|||
| Izod Impact, Notched |
6.86
J/cm <br>@Thickness 3.17 mm
|
12.9
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Samsung Cheil Industries Infino® NH-1035 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
|
|||
| Izod Impact, Notched |
6.86
J/cm <br>@Thickness 3.17 mm
|
12.9
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Samyang Trirex® 3017PJ Polycarbonate
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017PJ is a super high flow grade.Information provided by Samyang.
|
|||
| Izod Impact, Notched |
6.90
J/cm <br>@Temperature 23.0 °C
|
12.9
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
Styron CALIBREâ„¢ 891-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release..
|
|||
| Izod Impact, Notched |
6.90
J/cm <br>@Temperature 23.0 °C
|
12.9
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
Styron CALIBREâ„¢ 893-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 893-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release..
|
|||
| Izod Impact, Notched |
6.86
J/cm <br>@Thickness 3.17 mm
|
12.9
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Samyang Trirex® 3017IR Polycarbonate with Heat Stabilizer
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017IR is a super high flow grade with added heat stabilizers, separating materials and..
|
|||
| Izod Impact, Notched |
6.90
J/cm <br>@Thickness 3.20 mm
|
12.9
ft-lb/in <br>@Thickness 0.126 in
|
ASTM D256 |
|
Covestro Bayblend® T 85 Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 ..
|
|||
| Izod Impact, Notched |
6.90
J/cm <br>@Thickness 3.17 mm
|
12.9
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Covestro Makrolon® 6255 Polycarbonate, Flame Retardant, High Productivity, Mold Release
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
|
|||
| Izod Impact, Notched | 6.86 J/cm | 12.9 ft-lb/in | ASTM D256 |
|
E-Polymers TEKAMID® H14HR High Toughness Heat Resistance PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..
|
|||
| Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
|
ABW Polymers PC/PET Alloy
Typical property data below. Material may be tailored to meet specific requirements. This data should be used only as a guide and no assurance can be granted by the company that all molded articles..
|
|||
| Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
|
E-Polymers Tekaloy® S630X , High Impact, Weather Resistance, Chemical Resistance PC/PBT Alloy
High impact, weather resistance, chemical resistanceInformation provided by E-Polymers Co. Ltd.
|
|||