Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 14.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.07 - 7.47 J/cm
2.00 - 14.0 ft-lb/in
ASTM D256
Novatec Novacycle® 501 PVC
Novacycle® 501 is a general purpose, rigid, extrusion grade PVC compound in pellet form. This formulation is designed to provide an economical alternative for extruded profiles Raw material appe..
Izod Impact, Notched 0.374 - 7.47 J/cm
0.700 - 14.0 ft-lb/in
Average value: 1.94 J/cm Grade Count:22
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..
Izod Impact, Notched 0.267 - 7.47 J/cm
0.500 - 14.0 ft-lb/in
Average value: 1.04 J/cm Grade Count:76
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Izod Impact, Notched 0.267 - 7.47 J/cm
0.500 - 14.0 ft-lb/in
Average value: 2.11 J/cm Grade Count:18
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Izod Impact, Notched 0.290 - 7.47 J/cm
0.543 - 14.0 ft-lb/in
Average value: 0.937 J/cm Grade Count:73
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Izod Impact, Notched 4.27 - 7.47 J/cm
8.00 - 14.0 ft-lb/in
ASTM D256
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Izod Impact, Notched 0.534 - 7.47 J/cm

@Temperature -40.0 - 0.000 °C
1.00 - 14.0 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 3.11 J/cm Grade Count:4
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Izod Impact, Notched 0.534 - 7.47 J/cm

@Thickness 3.18 - 3.18 mm
1.00 - 14.0 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 3.11 J/cm Grade Count:4
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Izod Impact, Notched 4.81 - 7.47 J/cm
9.00 - 14.0 ft-lb/in
ASTM D256
Premix Premi-Glas® 1200H-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni..
Copyright © lookpolymers.com All Rights Reserved