| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
1.10
J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
|
PolyOne LubriOne™ NI-0920063 NATURAL Polyamide 610 (Nylon 610)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Izod Impact, Notched |
1.10
J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
|
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
|
|||
| Izod Impact, Notched |
1.10
J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
|
PolyOne Nymax™ ND633 GF Black Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | |
|
Owens Corning Glass Fiber Reinforced Polyurethane, Flaked Glass (RRIM), 23 wt.% glass
Polyurethane is normally used for its structural properties when molded. It is highly resistant to most organic solvents. It is not recommended for use with strong acids and alkalis, steam, fuels, a..
|
|||
| Izod Impact, Notched |
1.10
J/cm @Temperature -30.0 °C |
2.06
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® 915AU PC (Europe-Africa-Middle East)
LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte..
|
|||
| Izod Impact, Notched |
1.10
J/cm @Temperature -30.0 °C |
2.06
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific)
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA)
(Unverified Data**)
Amodel AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**)
AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. ..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | reverse notched; ASTM D256 |
|
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer
(discontinued **)
Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® BFL2010 PC (Europe-Africa-Middle East)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors.
|
|||
| Izod Impact, Notched |
1.10
J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.06
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
|
PolyOne Geon™ 80530 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Izod Impact, Notched |
1.10
J/cm @Temperature -30.0 °C |
2.06
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer
|
|||
| Izod Impact, Notched |
1.10
J/cm @Thickness 3.17 mm |
2.06
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Izod Impact, Notched |
1.10
-
4.90
J/cm @Thickness 0.800 - 3.17 mm |
2.06
-
9.18
ft-lb/in @Thickness 0.0315 - 0.125 in |
Average value: 2.67 J/cm Grade Count:3 |
|
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256A |
|
LyondellBasell Astryn BA45H Polypropylene Copolymer, Flame Retardant
Key Features: medium melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colorability..
|
|||
| Izod Impact, Notched |
1.10
J/cm @Temperature 0.000 °C |
2.06
ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East)
VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage.
|
|||
| Izod Impact, Notched |
1.10
J/cm @Temperature -40.0 °C |
2.06
ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
|
Sterigenics Raprex® R-100 Branched High Density Polyethylene
Applications: ExtrusionRAPREX® R-100 is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched struct..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
|
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Izod Impact, Notched |
1.10
J/cm @Thickness 3.20 mm |
2.06
ft-lb/in @Thickness 0.126 in |
ASTM D256 |
|
Supreme Petrochem SP 564 Flame Retardant Polystyrene
Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxes, ele..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ISO 180 |
|
Wellman Wellamid® GF33-66 XE-N, 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Izod Impact, Notched |
1.10
J/cm @Temperature 23.0 °C |
2.06
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram RamTough RZ300G3 Polycarbonate, 15% Glass Fiber
15% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
|
Toyobo T-422-02R Nylon, Mineral-Reinforced
Key Feature: High heat distortion and good toughness, high flowInformation provided by Toyobo Co., Ltd
|
|||
| Izod Impact, Notched |
1.10
J/cm @Temperature 23.0 °C |
2.06
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
Cossa Polimeri ESTACARB 0820 GF V0 HF Flame Retardant Polycarbonate
Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, antimony, chlorine and bromine free, high stiffness, high dimensional stability, good processability, good light resistanceI..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
|
E-Polymers SEPAZ® N6030FR 30% Glass Fiber Reinforced Flame Retardant Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
|
Adell BR-37 Nylon 6, 35% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Izod Impact, Notched |
1.10
J/cm @Thickness 3.17 mm |
2.06
ft-lb/in @Thickness 0.125 in |
ASTM Test |
|
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d..
|
|||
| Izod Impact, Notched |
1.10
J/cm @Temperature -40.0 °C |
2.06
ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
|
Ashley Polymers Ashlene® D925 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl..
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256 |
|
Adell ER-38 Homopolymer Polypropylene, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Izod Impact, Notched | 1.10 J/cm | 2.06 ft-lb/in | ASTM D256A |
|
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer
Key Features: fast crystallization shortens cycle times, excellent cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: automotive blow molded partsMeets FDA requir..
|
|||