Polymer Property : Izod Impact, Notched = 2.25 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Packaging 2710 Amber 9360 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Packaging 2710 Amber 9375 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Packaging XPL 293 FROST 1733 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Izod Impact, Notched 1.20 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS
Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1...
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D412
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ GF 1200 A 40 IM Black 13A Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East)
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
23° C; ASTM D256
Flint Hills AP5325-HS Impact Copolymer Polypropylene
High impact copolymer, UL certified, and FDA compliant. Features: Nucleated and heat stabilizedApplications: Injection molding: large, thin wall automotive interior parts.Former Huntsman polypropyle..
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256-03
Ipiranga Petrochem GD 5160 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha..
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry)
Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA
NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability.
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific)
NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability.
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
Izod Impact, Notched 1.20 J/cm

@Thickness 3.20 mm
2.25 ft-lb/in

@Thickness 0.126 in
ASTM D256
Supreme Petrochem SH 2114 High Impact Polystyrene
Characteristics Very high impact strength Easy processing High heat Processing Extrusion MoldingApplications Toys, shoe heels, cosmetic boxes, pill vials Luggage cases Blending with clear polys..
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Asia Pacific)
Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Asia Pacific)
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamSter PF300G6 PBT, 30% Glass Fiber
30% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamOfin PPC364I6 Polypropylene, 30% Mineral and Glass Fiber
30% mineral and glass fiber reinforced, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched >= 1.20 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 2.25 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
EPICHEM Epilac ABS-BLACK Acrylonitrile Butadiene Styrene
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D 256
Cossa Polimeri ESTABIO PL 0560 T10 Biodegradable Plastic
Biodegradable plastic for the extrusion of disposablesCertified for food contactInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Adell BT-13 Nylon 6, 15% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamSter PF392G6 PBT, 30% Glass Fiber
30% glass-fiber reinforced, surface modified PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256A
LyondellBasell Astryn 73A6-3 Polypropylene Copolymer, 30% Calcium Carbonate
Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, excellent aesthetics, high gloss, ..
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ISO 180
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH) &nbsp
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..