| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
4.00
J/cm <br>@Temperature 23.0 °C
|
7.50
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Izod Impact, Notched |
4.00
J/cm <br>@Temperature 23.0 °C
|
7.50
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Izod Impact, Notched |
4.00
J/cm <br>@Temperature 23.0 °C
|
7.50
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
|
NCMT NanoPAC™ S202 High Performance Polypropylene Nanocomposite
Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
|
NCMT NanoPAC™ S222 High Performance Polypropylene Nanocomposite
Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics GELOY CR8510 ASA
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
|
|||
| Izod Impact, Notched |
>=
4.00
J/cm <br>@Temperature 23.0 °C
|
>=
7.49
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East)
Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p..
|
|||
| Izod Impact, Notched |
4.00
J/cm <br>@Temperature -30.0 °C
|
7.49
ft-lb/in <br>@Temperature -22.0 °F
|
ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Europe-Africa-Middle East)
Cycoloy Medium Heat Plating Grade for Automotive
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East)
High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only.
|
|||
| Izod Impact, Notched |
4.00
J/cm <br>@Temperature -20.0 °C
|
7.49
ft-lb/in <br>@Temperature -4.00 °F
|
ASTM D256 |
|
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)
(discontinued **)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
|
Gichem GIBLEND E45400 Polycarbonate / ABS
(discontinued **)
Polycarbonate and ABS blend, high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® LUX9612 PC (Asia Pacific)
Lexan LUX9612 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | Partial Break; ASTM D256 |
|
Ineos G36-24-149 MDPE with Carbon Black
(discontinued **)
Fortiflex® G36-24-149 is a black medium density polyethylene resin designed for sheet extrusion. This resin has excellent environmental stress crack resistance (ESCR) and ultra violet protection. ..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | Reverse notched; ASTM D256 |
|
LG Chemical LUCEL MR-310 Low Warpage POM, 10% Mineral Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | Partial break |
|
Ineos G36-24-150 HDPE
Ineos G36-24-150 is a medium density polyethylene resin designed for geomembrane sheet extrusion. The resin has excellent environmental stress crack resistance (ESCR).Natural resin; some physical p..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
|
Metton LMR M1539 Liquid Molding Resin
Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can ..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256-93a |
|
Multibase Multi-ABS 802 Natural Extrusion Grade
Data provided by Multibase.
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256A |
|
LyondellBasell Astryn BB725GC Polypropylene Copolymer, Mineral Filled
Key Features: medium melt flow, medium high modulus, UV-stabilized, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good processability, good weatherability,Applicati..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | 73°F; ASTM D256 |
|
Spartech Royalite R26 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM Data |
|
Styron Magnumâ„¢ 9035 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | -20°F; ASTM D256 |
|
Styron Pulse® 2200BG ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Izod Impact, Notched |
4.00
J/cm <br>@Thickness 3.20 mm
|
7.49
ft-lb/in <br>@Thickness 0.126 in
|
reverse notched; ASTM D 256 |
|
SABIC Innovative Plastics Ultem 2110N PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
|
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
|
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.50 ft-lb/in | ASTM D256 |
|
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
|
|||
| Izod Impact, Notched |
4.00
J/cm <br>@Thickness 3.17 mm,<br> Temperature 23.0 °C
|
7.49
ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
Diamond Polymers ABS 6501 Injection Molding Grade, Extra High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Izod Impact, Notched |
4.00
J/cm <br>@Thickness 3.17 mm,<br> Temperature 23.0 °C
|
7.49
ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F
|
ASTM D256 |
|
Diamond Polymers ABS 9950 Injection Molding Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
|
E-Polymers TEKAMID® TB110HI , High Impact PA6, DAM