Mechanical Properties Metric English Comments
Izod Impact, Notched 0.694 - 2.67 J/cm
1.30 - 5.00 ft-lb/in
Average value: 1.16 J/cm Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Izod Impact, Notched 0.427 - 2.67 J/cm
0.800 - 5.00 ft-lb/in
Average value: 1.25 J/cm Grade Count:12
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a..
Izod Impact, Notched 0.320 - 2.67 J/cm
0.599 - 5.00 ft-lb/in
Average value: 0.817 J/cm Grade Count:86
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched 0.534 - 2.67 J/cm
1.00 - 5.00 ft-lb/in
Average value: 0.778 J/cm Grade Count:21
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Notched 0.600 - 2.67 J/cm
1.12 - 5.00 ft-lb/in
Average value: 1.60 J/cm Grade Count:10
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched 0.427 - 2.67 J/cm
0.800 - 5.00 ft-lb/in
Average value: 1.16 J/cm Grade Count:27
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.481 - 2.67 J/cm
0.900 - 5.00 ft-lb/in
Average value: 1.10 J/cm Grade Count:15
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Notched 2.14 - 2.67 J/cm
4.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC 1603 Multi-purpose grade
BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160..
Izod Impact, Notched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact
BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap..
Izod Impact, Notched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC 605LWR Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 605LWR is a mineral filled, glass fiber reinforced polyester bulk molding compound suitable for compression, transfer and stuffer injection molding. It is designed to provide improved wear resis..
Izod Impact, Notched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl..
Izod Impact, Notched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC
BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab..
Izod Impact, Notched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC SLC 1000 Glass Reinforced Polyester
BMC SLC 1000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. It is V-0 flame arc and track resistant. UL® recognized. This material was formerly known..
Izod Impact, Notched 1.07 - 2.67 J/cm
2.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC 1100 Corelyn Glass Fiber Reinforced Polyester Compound
BMC 1100, also known as CoreLyn, is a food contact safe material with excellent scratch and stain resistant properties. CoreLyn can be pigmented to match virtually any color. This glass fiber-reinfo..
Izod Impact, Notched 2.14 - 2.67 J/cm
4.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC 5307 Mineral Filled, Glass Reinforced Polyester
BMC 5307 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a medium impact material produced in ..
Izod Impact, Notched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC 6605A Polyester Molding Compound
Izod Impact, Notched 0.210 - 2.67 J/cm
0.393 - 5.00 ft-lb/in
Average value: 0.768 J/cm Grade Count:93
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched 1.62 - 2.67 J/cm

@Temperature 23.0 °C
3.03 - 5.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Kleerdex Kydex® 115 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
High rigidity sheet for ceiling panelsApplications: Ceiling panels in clean rooms, computer rooms, laboratories, food, dairy, and pharmaceutical plants, and other environments where a high degree of..
Izod Impact, Notched 1.60 - 2.67 J/cm
3.00 - 5.00 ft-lb/in
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound
BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific ..
Copyright © lookpolymers.com All Rights Reserved