Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 5.34 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Asia Pacific)
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
Izod Impact, Notched 5.34 J/cm

@Temperature 22.8 °C
10.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow
PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
Izod Impact, Notched 5.34 J/cm

@Temperature 22.8 °C
10.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Izod Impact, Notched 5.34 J/cm

@Temperature 22.8 °C
10.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:..
Izod Impact, Notched 5.34 J/cm

@Temperature -30.0 °C
10.0 ft-lb/in

@Temperature -22.0 °F
0.125in; ASTM D256
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate
Information provided by Ravago
Izod Impact, Notched 5.34 J/cm

@Temperature 22.8 °C
10.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade
PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 22% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Izod Impact, Notched 5.34 J/cm

@Temperature -18.0 °C
10.0 ft-lb/in

@Temperature -0.400 °F
ASTM D4812
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade
ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c..
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
at 73°F; ASTM D256
M. Holland Company CP510 Polypropylene Copolymer
Additives: Heat Stabilizer, Nucleating AgentsFeatures: High Flow, High Impact Resistance, Heat Stabilizer, NucleatedUses: Construction Applications, Lawn and Garden EquipmentApprovals: FDA 21 CFR 17..
Izod Impact, Notched 5.34 J/cm

@Thickness 3.20 mm
10.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM AR9300 PEI (Asia Pacific)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
73°F, 0.125 in.; ASTM D256
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS
Information provided by Star Plastics, Inc.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM Data
Styron Pulse® 1310 ABS + Polycarbonate
PULSE® 1310 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing..
Izod Impact, Notched 5.34 J/cm

@Temperature -50.0 °C
10.0 ft-lb/in

@Temperature -58.0 °F
ASTM Data
Styron Pulse® 1370 ABS + Polycarbonate
PULSE® 1370 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing..
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
-20°F; ASTM D256
Styron Pulse® 2000 ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Izod Impact, Notched 5.34 J/cm

@Temperature -30.0 °C
10.0 ft-lb/in

@Temperature -22.0 °F
0.125 in; 10 mil notch; ASTM D256
Styron CALIBREâ„¢ IM 401-11 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM Data
Styron Magnumâ„¢ 1040 ABS, Very High impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
A. Schulman PP 1500X-01 Polypropylene High Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1500X-01 is a specially formulated high impact copolymer polypropylene.Information provided by A. Schulman.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
A. Schulman ComAlloy® E-12672 Polyester Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
A. Schulman PP 1500X-01 Polypropylene High Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1500X-01 is a specially formulated high impact copolymer polypropylene.Information provided by A. Schulman.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
A. Schulman PP 1692 Polypropylene High Impact Copolymer
DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene
DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
A. Schulman ComAlloy® E-12672 Polyester Alloy
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app..
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers DIAMALOY 750 HF PLATABLE ABS/PC Alloy, Platable Non-Halogen, Flame Retardant
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Colorite Polymers 2018 Rigid PVC
Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ..
Izod Impact, Notched 5.34 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
10.0 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 5.34 - 8.01 J/cm
10.0 - 15.0 ft-lb/in
ASTM D256
Premix Premi-Glas® 1200-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa..
Copyright © lookpolymers.com All Rights Reserved