| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
6.40
J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
|
PolyOne Maxxam™ FR PP FR 7B31 Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
|
|||
| Izod Impact, Notched |
6.40
J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.0
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
|
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid)
Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: ..
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
Quantum Composites QC-2150 50% Glass Reinforced Phenolic SMC
QC-2150 is a glass reinforced phenolic engineered structural composite molding compound. It exhibits outstanding low flammability characteristics. QC-2150 is recommended for applications such as a..
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® 950 PC
Opaque colors, high viscosity, superior flame retardance.
|
|||
| Izod Impact, Notched |
6.40
J/cm @Thickness 6.40 mm |
12.0
ft-lb/in @Thickness 0.252 in |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| Izod Impact, Notched |
6.40
J/cm @Thickness 6.40 mm |
12.0
ft-lb/in @Thickness 0.252 in |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Asia Pacific)
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| Izod Impact, Notched |
6.40
J/cm @Temperature -30.0 °C |
12.0
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® HF1140R PC
High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib..
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® ML4506 PC
Transparent polycarbonate for aircraft applications requiring FAR 25.853a compliance. Injection moldable.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® PC2200 PC (Asia Pacific)
PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific)
High impact and ductility at 73F (23C) and -20F (-29C).
|
|||
| Izod Impact, Notched |
6.40
J/cm @Thickness 6.40 mm |
12.0
ft-lb/in @Thickness 0.252 in |
ASTM D256 |
|
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® HF1110R PC
High flow grade. Easy mold release version of LEXAN HF1110. For thin wall lighting lenses, data storage components and safety eyewear lenses.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | natural, tints; ASTM D256 |
|
SABIC Innovative Plastics Lexan® HF1140 PC
Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this..
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® HF1140 PC (Asia Pacific)
Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors. Effective January 15th, 2007 th..
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® HF1140 PC (Europe-Africa-Middle East)
Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this..
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® ML4248 PC
Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Extrusion grade. Transparent, transluscent and opaque colors.
|
|||
| Izod Impact, Notched |
6.40
J/cm @Thickness 3.17 mm |
12.0
ft-lb/in @Thickness 0.125 in |
ASTM D256 |
|
Covestro Apec® DP9-9333 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® SFX173RU PC
SFX173RU is a transparent SecurFX grade with high flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | edgewise; ASTM D256 |
|
Haysite HST-II Glass Reinforced Polyester Sheet, Electrical Grade
UL, Inc. has granted HST-II the highest thermal recognition ever achieved by any glass polyester laminate (U.L. File No. E81893). HST-II has a 220º C/210º C rating for 1/8" thick and heavier,..
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics PC2200 PC (Asia Pacific)
PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East)
PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® 365 PET (Asia Pacific)
Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"".
|
|||
| Izod Impact, Notched |
6.40
J/cm @Temperature -20.0 °C |
12.0
ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
|
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East)
PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ PP 7001
Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ PP 7001
Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ PP 7001
Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
A. Schulman POLYFORT™ PP 7001
Information provided by A. Schulman.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | |
|
Cosmic Plastics CP7314 Epoxy Molding Compound
Data provided by the manufacturer.
|
|||
| Izod Impact, Notched | 6.40 J/cm | 12.0 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® 940 PC (Asia Pacific)
Opaque colors, medium viscosity, superior flame retardance.
|
|||