| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® 905AU PC (Asia Pacific)
LEXAN resin grade 905AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in all colors, intended to ..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® PC1800 PC (Asia Pacific)
PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® PC1800R PC (Asia Pacific)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors.
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1025/9..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® VR2020 PC (Europe-Africa-Middle East)
VR2020 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched |
>=
7.00
J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>=
13.1
ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
|
Kingfa LONOY 1300 PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | Reverse notched; ASTM D256 |
|
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Izod Impact, Notched |
7.00
J/cm @Temperature 23.0 °C |
13.1
ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
|
Lavergne VYTEEN PC 135 General Purpose Medium Viscosity Polycarbonate
Vyteen PC 135, Black, medium viscosity polycarbonate, has an excellent balance of stiffness and impact resistanceFeatures: - High heat resistance - Good processabilityInformation provided by Biegl..
|
|||
| Izod Impact, Notched |
7.00
J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
13.1
ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
|
Kingfa PC-WT01 Weather Resistance PC
Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec..
|
|||
| Izod Impact, Notched |
7.00
J/cm @Temperature 23.0 °C |
13.1
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics PC1800 PC (Asia Pacific)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
|
|||
| Izod Impact, Notched |
7.00
J/cm @Temperature 23.0 °C |
13.1
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics PC1800R PC
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics PC1800R PC (Asia Pacific)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched |
7.00
J/cm @Temperature 23.0 °C |
13.1
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics PC1803R PC
PC1803R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Xenoy® X4820 PBT+PC
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific)
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
Styrolution Luran® S KR 2863 C Colored ASA+PC
Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
Styrolution Luran® S KR 2864 C Colored ASA+PC
Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr..
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
Styrolution Luran® S KR 2864 C UV Colored ASA+PC
Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr..
|
|||
| Izod Impact, Notched |
7.00
J/cm @Temperature 23.0 °C |
13.1
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram RamTough PZ741 Polycarbonate, UV Stabilized
UV stabilized low viscosity polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Izod Impact, Notched |
7.00
J/cm - NB @Temperature 23.0 °C |
13.1
ft-lb/in - NB @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram RamTough RZ224 Polycarbonate, Injection Molding
Polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
|
Styrolution Luran® S KR 2863 C UV Colored ASA+PC
Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
|
|||