| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
3.74
J/cm <br>@Temperature 23.0 °C
|
7.00
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Izod Impact, Notched |
3.74
J/cm <br>@Temperature 23.0 °C
|
7.00
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
RheTech Products FT7016-50UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Izod Impact, Notched |
3.74
J/cm <br>@Temperature 22.8 °C
|
7.00
ft-lb/in <br>@Temperature 73.0 °F
|
ASTM D256 |
|
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized
Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
|
|||
| Izod Impact, Notched |
3.74
J/cm <br>@Temperature -30.0 °C
|
7.00
ft-lb/in <br>@Temperature -22.0 °F
|
0.125in; ASTM D256 |
|
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate
Information provided by Ravago.
|
|||
| Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | ASTM D256 |
|
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
|
|||
| Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | ASTM D256 |
|
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound
The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl..
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
|
Global ABS-704 General Purpose High Impact ABS
Information provided by Global Polymers Corporation.
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
|
Multibase Multi-Flex® D 6500 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant General PurposeDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Blow Molding Uses: Automotive Applica..
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | 73°F; ASTM D256 |
|
Spartech Royalite R21 ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | 73°F; ASTM D256 |
|
Spartech Royalite R84/21 Weather Resistant Sheet
Description: Weather Resistant SheetInformation provided by Spartech.
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | 73°F; ASTM D256 |
|
Spartech Royalite R87/59 ABS/PVC Weather Resistant Sheet
Description: Weather Resistant SheetInformation provided by Spartech.
|
|||
| Izod Impact, Notched |
3.74
J/cm <br>@Thickness 3.17 mm
|
7.00
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
|
Star Plastics ABS405 Extrusion Grade ABS
Information provided by Star Plastics, Inc.
|
|||
| Izod Impact, Notched |
3.74
J/cm <br>@Temperature -30.0 °C
|
7.00
ft-lb/in <br>@Temperature -22.0 °F
|
0.125 in; 10 mil notch; ASTM D256 |
|
Styron CALIBREâ„¢ IM 401-18 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | 0.125 in; ASTM D256 |
|
Chase Plastics CP Pryme® APC300 ABS Polycarbonate Alloy, Recycled Content
Features: Recycled contentForm: PelletsInformation provided by Chase Plastics.
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D628 |
|
ACC EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy
EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast..
|
|||
| Izod Impact, Notched | 3.74 - 4.27 J/cm | 7.00 - 8.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength
BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat..
|
|||
| Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | |
|
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound
BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar..
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D628 |
|
ACC EP QS EPI Engineered Polymers Quick Set Epoxy
EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure..
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D256 |
|
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Izod Impact, Notched | 3.74 J/cm | 7.00 ft-lb/in | Partial Break; ASTM D256 |
|
Ineos HB111R Polyethylene Copolymer
HB111R is a natural high molecular weight, high-density copolymer polyethylene developed for automotive fuel tanks. It combines excellent processability and outstanding physical performance, particu..
|
|||
| Izod Impact, Notched |
3.74
J/cm <br>@Thickness 3.17 mm
|
7.00
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES HiFill® TPU 0600
Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc.
|
|||