| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
STN EN ISO 179 |
|
Plastcom PLASTAMID® 66 GF 30 PA66 reinforced with glass fiber
PA66 for injection molding, reinforced with 30% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
STN EN ISO 179 |
|
Plastcom SLOVAMID 6 GF 15 Polyamide 6, 15% Glass Fiber
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycolac® S705 ABS (Europe-Africa-Middle East)
CYCOLAC S705 is a new generation ABS plating grade, offering semi high heat with a good property balance for impact and flow. CYCOLAC S705 demonstrates excellent electroplatability and a good therma..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYfill PP EQX10030R UV Polypropylene, Mineral Reinforced, Modified
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYfill PPH GF5020 PD1 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polykemi AB SCANAMID 66 A13^ F15 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polykemi AB SCANTEC PC S60R GF30 V0 Polycarbonate, Glass-Fiber Reinforced, Flame Retardant
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
PolyOne Bergamid™ A700 BK VN4255 LS Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYfill PPH BF4075 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
DSM Akulon® S223-E Nylon 66 (European and Asian Grade) (Cond)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
LG Chemical LI-913 ASA, Injection Molding, High Impact
Information Provided by LG Chem
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179/1eA |
|
Inno-Comp INNOPOL® CS 2-3302 Elastomer Modified Polypropylene Block-Copolymer
INNOPOL® CS 2-3302 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-3302 is developed for produ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Inno-Comp INNOPOL® CS 2-4120 20% Talc-Filled Polypropylene Block-Copolymer
INNOPOL® CS 2-4120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form as well.INNOPOL® CS 2-4120 is developed for p..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East)
VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Styrolution Terblend® N NG-02 EF 8% Glass Filled ABS+PA (Conditioned)
Description: Terblend® N NG-02 EF is a glass fiber reinforced UV stabilized ABS/PA blend with excellent dimensional stability and high impact strength. The enhanced flowability enables excellent ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® S223-D (Dry) Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® S223-D Nylon 66 (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/eA |
|
Eurotec® Tecomid® NA40 KK30 NL PA 6.6 30% glass fiber/mineral reinforced, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
DSM Arnite® B434 SE PBT-GF20 FR(17)
20% Glass Reinforced, Flame Retardant
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
BASF Ultraform® S2320 0035 LEV POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
BASF Ultraform® W2320 U035 LEV POM
Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, Conditioned
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
DSM Akulon® K225-KS (Cond.) Flame Retardant (Halogen free), Heat Stabilized Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80x10x4 sp=62; ISO 179/1eA |
|
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded
BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM
Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and..
|
|||