| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Plastcom SLOVALEN PC 59 GF 30 PP, 30% glass fibre
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains themodifier of mechanical properties.Increased strength in comparison with unfilled PP. A..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -20.0 °C
|
3.81
ft-lb/in² <br>@Temperature -4.00 °F
|
STN EN ISO 179 |
|
Plastcom SLOVAMID 6 GF 35 Polyamide 6, 35% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 35% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Plastcom SLOVAMID 6 NG1 GF 20 HLS PA6, 20% glass fibre, combined stability
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre, heat and wheather stabilized. Stabilized against hydrolisys. Good surface finisch. Scratch resistent.Packaging, tra..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -20.0 °C
|
3.81
ft-lb/in² <br>@Temperature -4.00 °F
|
STN EN ISO 179 |
|
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -20.0 °C
|
3.81
ft-lb/in² <br>@Temperature -4.00 °F
|
|
|
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre
FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/2C |
|
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East)
CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East)
CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East)
Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by ..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYasa 2008F UV-stabilized, High Flow ASA
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB POLYfill PPH GF12030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -20.0 °C
|
3.81
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polykemi AB POLYshine PBT D231 GF15 PBT, Glass-Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
>=
0.800
J/cm² <br>@Temperature 23.0 °C
|
>=
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
DIN 53453 |
|
Qualchem Danamid AFGFH-30 Polyamide 66, 30% Glass Fiber
Reinforced with glass fiber. Heat stabilized, for long-lasting use at 120-140°C.Information provided by Qualchem Zrt.
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
STN EN ISO 179 |
|
Plastcom SLOVAMID 6 GF 20 Polyamide 6, 20% Glass Fiber
FeaturesPA 6 for injection moulding, chemically coupled with 20% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and con..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -20.0 °C
|
3.81
ft-lb/in² <br>@Temperature -4.00 °F
|
STN EN ISO 179 |
|
Plastcom SLOVAMID 6 LI/1 Polyamide 6, Impacted
FeaturesPA 6 with the content of thermoplastic elastomer. Impacted, for mouldings with high toughness either at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Ultem ATX153R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Suzhou Hipro Polymers Hiprolon® 70 NN Nylon 610, conditioned
Hiprolon® 70 NN is medium viscosity polyamide 6.10 containing a bio-renewable resource. Features: low density, low water absorption, high dimension stability, high notched impact resistance, goo..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Polyram PlusTek PB826G3 Nylon 6 for Injection Molding, 15% Glass-fiber Reinforced, Impact Modified and UV Stabilized
15% Glass fiber reinforced, impact modified and UV stabilized Nylon 6 for injection molding applications.Information provided by Polyram.
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® K222-D Nylon 6 (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Arnite® TV6 240 PBT-GF20
20% Glass Reinforced
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, Conditioned
Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry)
Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Radici Radilon® S 38F (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Arnite® TV4 230 PBT-15% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Charpy Impact, Notched |
0.800
J/cm² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Sax Polymers SAXALEN PPH327G28 Polypropylene Homopolymer, 28% Glass Filled
SAXALEN PPH327G28 is a 28% glass filled Polypropylene - Homopolymer injection molding grade with increased stiffness.Information provided by SAX Polymers
|
|||