Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVALEN PH 69 GF 30 Polypropylene Homopolymer, 30% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
STN EN ISO 179
Plastcom SLOVAMID® 6 GF 30 FRG 2 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 30 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability in accordance with UL 94 5 at 3.2 mm. Application for the ..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East)
CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Polykemi AB SCANAMID 66 A13^ F30 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Durethan® B 30 S 000000 Nylon 6
PA 6, injection molding-grade, non-reinforced, easy-flow, easy-release, rapid solidification
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
Conditioned; ISO 179-1eA
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres
PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -40.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -40.0 °F
ISO 179-1eA
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres
PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
Conditioned; ISO 179/1eA
Lanxess Durethan® BKV 15 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
cond.; ISO 179-1eA
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow)
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Pocan® B 4215 000000 PBT, 12% Glass Fiber
PBT, 12% glass fibers, injection molding, flame retardant
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Pocan® B 7375 000000 PBT, White Pigment
PBT, 25% white pigments, injection molding, improved light reflection, low tendency to warp
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Pocan® BF 4215 000000 PBT, 12% Glass Fiber
PBT, 12% glass fibers, injection molding, flame retardant
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179-1eA
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral
PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS.
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;..
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Durethan® A 30 000000 Nylon 66
PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in..
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179-1eA
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral
PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber
PBT, 7% glass fibers, injection molding, flame retardant
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber
PBT, 7% glass fibers, injection molding, flame retardant
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® K225-KWS (Cond.) Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
DSM Stanyl® TS250F6D Nylon 46-30% Glass Reinforced (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® S223-G6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
Arkema Group Pebax® 7233 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7233 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
Conditioned; ISO 179/1eA
Lanxess Durethan® BKV 35 H2.0 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: automotive structures
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Pocan® B 3215 000000 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
dry; ISO 179/1eA
DSM Stanyl® TE300 PA46
Heat Stabilized
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region.