| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
|
Plastcom SLOVAMID 66 GF 35 FRI 3 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® FXC810AL PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810AL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Alpine White colour effects. The colour package may effect performance.This data was..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® FXE174R PC (Europe-Africa-Middle East)
LEXAN FXE174R is a high flow visualFx Energy grade, suitable for steam sterilization and compliant with medical and food contact regulations. This material is especially developed for applications t..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
DSM Arnite® TV4 460 KL TV4 460 PBT/PET Blend-30% Glass Reinforced (European Grade)
(discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
|
|
Plastcom SLOVALEN PC 93 T 30 PP reinforced with 30% mineral filler
Features: Modified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furni..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
|
|
Radici Radilon® S RV300R (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**)
Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by ..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
DSM Akulon® K224-HG5 (Dry) 25% Glass Reinforced Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
|
LG Chemical HF-350 ABS, High Flow, High Impact
Information Provided by LG Chem
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 179-1eA |
|
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
Compression Molded; ISO 179/2 |
|
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
Sax Polymers SAXAMID 226F7 Nylon 6.6, 35% Glass Fiber
SAXAMID 226F7 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 35% glass fibers. It has very high mechanical strength in combination with good impact resistance. It is char..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
|
DSM Akulon® K224-G6-FC BK00001 PA6-GF30
30% Glass Reinforced, Food Contact Grade
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
5.71
ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
|
Covestro Makrolon® 2256 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -40.0 °C |
5.71
ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612
Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
DSM Akulon® S223-G6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
|
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry)
Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS ..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
(Unverified Data**)
Zytel® FG77G33L NC010 is a 33% glass fiber reinforced polyamide 612 resin for injection molding. It has been developed for consideration for applications such as parts in the food industry.Informat..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature -30.0 °C |
5.71
ft-lb/in² @Temperature -22.0 °F |
ISO 179/eA |
|
Eurotec® Tecodur® PB70 GR45 NL PBT 45% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Charpy Impact, Notched |
1.20
J/cm² @Temperature 23.0 °C |
5.71
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry)