Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom PLASTALEN® PH 91 T 20 Polypropylene reinforced with mineral filler
Modified homopolymer PP for injection molding with the content of 20 % mineral filler. General application in all industry branches. Delivered in natural mode and in the full RAL color scale.Informa..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Plastcom PLASTAMID® 66 BT B 27 TS PA66 heat stabilized
Basic type PA66 for injection molding, heat stabilized, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - elec..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTAMID® 66 BT B 27 TS PA66 heat stabilized
Basic type PA66 for injection molding, heat stabilized, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - elec..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom SLOVAMID® 6 GF 25 E LS PA6 reinforced with glass fiber, UV stabilized
PA 6 grade for extrusion, reinforced with 25% glass fiber, determined for extrusion of window profile systems. Delivered in natural as well as full RAL scale color.Information Provided by Plastcom s..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVASTER® B1 BT TS PBT, basic type
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB SCANMID 6 B60 Nylon 6, Modified
Information provided by Polykemi AB
Charpy Impact, Notched 0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S CP300 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 0.350 - 0.500 J/cm²

@Temperature 23.0 °C
1.67 - 2.38 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group RALUPOL® 4806 UP
Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
PolyOne Bergamid™ B65 G/Mi20 UF grey LS Polyamide 6 (Nylon 6)
Information provided by PolyOne
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-2820 20% Glass-Fibre-Filled Polypropylene Homopolymer
INNOPOL® CS 1-2820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-2820 is recommended for producing in..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-5140 BLH is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-5140 BLH is recommended especially for producing products, where high stiffn..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Solvay TECHNYL® eXten D 437P PA6.10
Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis BF335SA Polypropylene Copolymer
BF335SA is a polypropylene copolymer intended for injection molding. This material has a very high impact strength while maintaining good stiffness, gives a good surface quality and is easy to proc..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis Daplen™ EE188HP Polypropylene TPO Compound
Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 0.000 °C
1.67 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
Borealis RA130E-1498 Polypropylene Random Copolymer
RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 0.000 °C
1.67 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
Borealis RA130E-6015 Polypropylene Random Copolymer
RA130E-6015 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust..
Charpy Impact, Notched 0.350 J/cm²

@Temperature 0.000 °C
1.67 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
Borealis RA130E-6017 Polypropylene Random Copolymer
RA130E-6017 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
BASF Ultraform® N2720 M210 POM
Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
BASF Ultraform® N2720 M210 POM
Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF
Charpy Impact, Notched 0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
BASF Ultraform® N2770 K POM
Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF
Charpy Impact, Notched 0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultramid® N-276 BK ND 3007 40% Glass/Mineral Filled PA66
Description: Ultramid N-276 BK ND3007 is a 40% mineral/glass reinforced, heat stabilized injection molding PA6/6.Information provided by BASF
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
BASF Ultraform® N2720 M63 30% Mineral Filled POM
Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant
High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid..
Charpy Impact, Notched 0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612  (Unverified Data**)
Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided..