Polymer Property : Charpy Impact, Notched = 2.14 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYabs T00 GF20 ABS, Glass Fibre-Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PPH GF5020 PD1 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A HSK (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S 32HS (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PPC 05ENH Polypropylene Copolymer, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PPC 200 E20 Polypropylene Copolymer, Elastomer Modified
Information provided by Polykemi AB
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB POLYfill PPH GF8030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66  (Unverified Data**)
Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® Ultraflow™ K-FHGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Cond)  (d
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 2-2120 20% Talc-Filled Polypropylene Block-Copolymer
INNOPOL® CS 2-2120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-2120 is developed for producing..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 2-3000 Polypropylene Block-Copolymer
INNOPOL® CS 2-3000 is a polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-3000 is developed for producing injection molded automot..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer
INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info..
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis BA390TF Polypropylene Copolymer
BA390TF is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA390TF is recommended for foam extrusion, or thermoforming.Inform..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Unipetrol PP MONSTEN® MA 745 Polypropylene Impact Copolymer
Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PP MONSTEN® MT 935 Polypropylene Random Copolymer
Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PP MONSTEN® MT 950 Polypropylene Random Copolymer
Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 11642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 60 g/10 min.Polypropylene PPC 11642 is characterized by high fluidity with good mechanical prope..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
Total PPC 4720XWZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4720XWZ is a nucleated impact copolymer with a Melt Flow index of 25 g/10 min.TOTAL Polypropylene 4720XWZ is characterized by improved stiffness, creep resistance,..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
Total PPC 4820WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h..
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
cond; ISO 179/1eA
DSM Stanyl® TW241B3 PA46-CF15
15% Carbon Reinforced, Heat Stabilized, Lubricated
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
DSM Stanyl® TW242FM10 PA46-(GF+MF)50
50% Glass/Mineral Reinforced, Heat Stabilized
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
BASF Ultraform® W2320 U03 POM
Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF
Charpy Impact, Notched 0.450 J/cm²

@Temperature -30.0 °C
2.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
BASF Ultraform® Z2320 003 POM
Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, ..
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPHC T8020 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 0.450 J/cm²

@Temperature 23.0 °C
2.14 ft-lb/in²

@Temperature 73.4 °F
Radici Radiflam® S RV250FR (dry) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..