| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
STN EN ISO 179 |
|
Plastcom PLASTALEN® PC 69 T 10 003/1M Polypropylene reinforced with mineral filler
Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o.
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
STN EN ISO 179 |
|
Plastcom PLASTAMID® 6 GF 30 005 PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 30% glass fiber, used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
|
|
Plastcom SLOVAMID 6 CF 20 PA6, 20% carbon fibre
FeaturesChemically reinforced with 20 % carbon fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry...
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polykemi AB SCANMID 6 B12^ F Nylon 6
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polykemi AB SCANMID 6 B12^ NH9 Nylon 6, Flame Retardant, Halogen Free
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Polykemi AB SCANTEC PC S60R GF20 V0 Polycarbonate, Glass-Fiber Reinforced, Flame Retardant
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB SCANMID 6 B12^ Q40 Nylon 6, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179/1eA |
|
Inno-Comp INNOPOL® CS 2-3302 Elastomer Modified Polypropylene Block-Copolymer
INNOPOL® CS 2-3302 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-3302 is developed for produ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
|
|
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179/1eA |
|
Borealis MG9647B Polyethylene
MG9647B is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Unipetrol PE HD LITEN® TB 38 HDPE
Made for tape applications.Information provided by Unipetrol RPA
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
DSM Akulon® S223-DH Nylon 66 (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
dry; ISO 179/1eA |
|
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80x10x4 sp=62; ISO 179/1eA |
|
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded
AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/eA |
|
Eurotec® Tecomid® NA40 KK30 NL PA 6.6 30% glass fiber/mineral reinforced, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/eA |
|
Eurotec® Tecomid® NB40 KK30 NL PA 6 30% glass fiber/mineral reinforced, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/eA |
|
Eurotec® Tecomid® NB40 NL XA 20 PA 6 unreinforced, UL94 V0
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
DSM Arnite® B434 SE PBT-GF20 FR(17)
20% Glass Reinforced, Flame Retardant
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179-1eA |
|
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced
PBT-GF10Information provided by BARLOG plastics GmbH.
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
BASF Ultraform® S2320 0035 LEV POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -40.0 °C
|
2.86
ft-lb/in² <br>@Temperature -40.0 °F
|
ISO 179 |
|
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, Conditioned
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, Conditioned
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, Conditioned
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
|
|||
| Charpy Impact, Notched |
0.600
J/cm² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179-1eA |
|
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
|
|||