Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 4.76 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -20.0 °C
4.76 ft-lb/in²
<br>@Temperature -4.00 °F
Plastcom SLOVALEN PC 11 N PP, imp. strength
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 30 006/1M PA6 reinforced with 30% glass fibre
Features: PA 6 for injection moulding, chemically strengthened with 30% of milled glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and cons..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
Plastcom SLOVAMID 66 GF 15 HI PA66, 15% glass fibre
FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -20.0 °C
4.76 ft-lb/in²
<br>@Temperature -4.00 °F
Plastcom SLOVAMID 66 GF 25 FRA 5 PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, reinforced with 25% glass fibre and halogen flame retardant. Application in electrical industry: breakers, coilforms, covers, terminals. Slightly decreased flam..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -20.0 °C
4.76 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 179
Polykemi AB POLYshine PBT D611 PBT
Information provided by Polykemi AB
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
Radici Radiflam® S RV300AE (cond.) Nylon 6
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPH GF8030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific)
DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® S223-G8U (Cond.) 43% Glass Reinforced Nylon 66 (North America) &nbsp;(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss
Information Provided by LG Chem
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
Conditioned; ISO 179/1eA
Lanxess Durethan® A 30 H2.0 901510 Nylon 66
PA 66 standard injection molding grade, non-reinforced, very easy release, good heat-ageing resistanceApplication Examples: terminal blocks, cable clips, bobbins, gearwheels
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -40.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -40.0 °F
d.a.m.; ISO 179-1eA
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
Conditioned; ISO 179/1eA
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of..
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
cond.; ISO 179-1eA
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
d.a.m.; ISO 179-1eA
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS.
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
d.a.m.; ISO 179-1eA
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS.
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Lanxess Pocan® B 1305 000000 PBT
PBT, non-reinforced, injection molding
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Lanxess Pocan® B 1700 000000 PBT
PBT, non-reinforced, extrusion, food contact
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature 23.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179-1eA
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral
PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS.
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance
Charpy Impact, Notched <= 1.00 J/cm²
<br>@Temperature -30.0 °C
<= 4.76 ft-lb/in²
<br>@Temperature -22.0 °F
Conditioned; ISO 179/1eA
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Styrolution PS 2710 HIPS
Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® S223-HG6 (Dry) 30% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® S223-HM8 (Cond.) 40% Mineral Reinforced, Heat Stabilized Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® S223-G6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
DIN ISO 179
BASF Elastollan R 2005/1 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P..