| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® C6850REC PC+ABS (Europe-Africa-Middle East)
PC+ABS Industrial quality. Flame retardant. Limited colors only (Black and Grey)This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
|
Polykemi AB POLYfill PP EIP5025 F VT2 Polypropylene, Mineral Reinforced, Extrusion grade, Low CLTE
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific)
6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® FXD101R PC (Europe-Africa-Middle East)
Transparent/translucent PC for light diffusion special effects. Thicker sections without sinks. Internal mold release. Pigment package may affect properties. Application testing always recommended..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle ..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -20.0 °C |
7.14
ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
|
Polykemi AB POLYlux 3809S PC/PBT-Blend
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region.
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179-1eA |
|
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eA |
|
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eA |
|
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers
PA 6, 50% glass fibers, injection molding, heat-ageing stabilized
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179-1eA |
|
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers
PA 6, 50% glass fibers, injection molding, heat-ageing stabilized
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
|
Lanxess Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
Styrolution Luran® S 778 TE Black 25991 ASA
Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Dry)
Description: Terblend® N NM-19 XP is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearanc..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -40.0 °C |
7.14
ft-lb/in² @Temperature -40.0 °F |
ISO R179 |
|
Styron Pulse® A20-95 PC/ABS
A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
|
DSM Akulon® K224-PG2 PA6-I-GF8
8% Glass Reinforced, Impact Modified
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
DSM Arnitel® EM740 74 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 70G35NOX BK309 Nylon 66
Zytel® 70G35NOX BK309 is a 35% glass reinforced, polyamide 66 resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution.Information provided by DuP..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eA |
|
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded
Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
|
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, Conditioned
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Dry, 23% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**)
Zytel® FG408L NC010 is a general purpose, lubricated, impact modified polyamide 66 resin with superior toughness for injection molding applications. It has been developed for consideration into app..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature 23.0 °C |
7.14
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
|
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, Conditioned
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
|
|||
| Charpy Impact, Notched |
1.50
J/cm² @Temperature -30.0 °C |
7.14
ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
|
|||