Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 8.09 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYabs P0P ABS, Plating Grade
Information provided by Polykemi AB
Charpy Impact, Notched 1.70 J/cm²

@Thickness 102 mm,
Temperature 23.0 °C
8.09 ft-lb/in²

@Thickness 4.00 in,
Temperature 73.4 °F
ISO 179
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound
PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS..
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Polykemi AB POLYabs F00 ABS
Information provided by Polykemi AB
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer
EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region.
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® ML3041 PC (Europe-Africa-Middle East)
LEXAN ML3041 has been developed for the injection moulding of thin-wall, complex parts that require high mechanical properties and impact resistance.This data was supplied by SABIC-IP for the Europe..
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® S223-PG2U (Dry) 13% Glass Reinforced, Impact Modified Nylon 66 (North America)  (discontinued **)&
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® K224-PG6U (Cond.) 33% Glass Reinforced, Impact Modified Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)
Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.I..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity..
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 179-1eA
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber
PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS.
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Novodur® HH-106 ABS
Novodur HH-106 is a high heat injection molding grade providing a balanced property profile.Information provided by Styrolution
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
Injection Molded; ISO 179/1eA
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines..
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eA
Styron Magnumâ„¢ 3525 Acrylonitrile Butadiene Styrene (ABS)
MAGNUMâ„¢ 3525 is a resin with excellent processing characteristics. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent processability with a stable..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber
SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce..
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Sax Polymers SAXAMID 236F4Q32 Nylon 6.6, 20% Glass Fiber
SAXAMID 236 F4Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers and very good flow properties. It is suitable for applications requiring toughness in co..
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
DSM Stanyl® OCD2300 BLK PA46-GF50
50% Glass Reinforced, Heat Stabilized
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Hytrel® G5564 TPC-ET  (Unverified Data**)
Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon ..
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4 sp=62; ISO 179/1eA
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Charpy Impact, Notched 1.70 J/cm²

@Temperature -20.0 °C
8.09 ft-lb/in²

@Temperature -4.00 °F
After conditioning at 23°C/50%RH; ISO 179/Af
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy
Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM
Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66  (Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Eurotec® Tecomid® NB40 KK30 NL IL PA 6 30% glass fiber/mineral reinforced, impact modified, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Charpy Impact, Notched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Charpy Impact, Notched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East)
High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.