Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 10.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -40.0 °C
10.9 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL B63 KF30 Nylon 6 for injection molding, 30% short glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -40.0 °C
10.9 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL B63 W-KF30 Nylon 6 for injection molding, 30% short glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -40.0 °C
10.9 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit RECONYL B GV30 Recycled nylon 6 for injection molding, 30% glass fiber reinforced
Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.30 - 8.00 J/cm²
10.9 - 38.1 ft-lb/in²
Average value: 4.42 J/cm² Grade Count:44
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Charpy Impact Unnotched 2.30 - 7.50 J/cm²

@Temperature -30.0 - -20.0 °C
10.9 - 35.7 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 4.35 J/cm² Grade Count:21
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Charpy Impact Unnotched 2.30 J/cm² - NB
10.9 ft-lb/in² - NB
Average value: 5.37 J/cm² Grade Count:20
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 2.30 - 6.80 J/cm²
10.9 - 32.4 ft-lb/in²
Average value: 4.31 J/cm² Grade Count:17
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.30 - 9.00 J/cm²
10.9 - 42.8 ft-lb/in²
Average value: 5.30 J/cm² Grade Count:10
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 20-7314 Polyphthalamide, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 20-7927 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned
Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi..
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
Charpy Impact Unnotched 2.30 J/cm²

@Temperature -30.0 °C
10.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/2C
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179-1
Unitika A1022GFL15 PA6, 15% Glass Fiber Reinforced, Dry
Information provided by Unitika Ltd.
Charpy Impact Unnotched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179; DIN 53453
Zell-Metall Engineering Plastics Zellamid 1400T (PET + solid lubricant)
Zellamid® 1400 is the registered trademark of Zell-Metall’s partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, ..
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL BK083 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179/IeU
Addiplast Addilene H 530 N30 Polypropylene Homopolymer
Good surface appearanceInformation provided by Addiplast.
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
Conditioned; ISO 179/IeU
Addiplast Addilene PMD 50272 Flame Retardant Polypropylene
Flame retardant, high rigidityInformation provided by Addiplast.
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179-1eU
Barlog Plastics KEBATRON C2065X3 PPS, cross-linked, 65% glass fiber / mineral reinforced, reduced residual chlorine
PPS-GF/MD 65Information provided by BARLOG plastics GmbH.
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
Arkema Group Appryl® HXN 1240 Polypropylene, 40% Talc Filled
Compound of a PP homopolymer and 40% talc, warm stabilized suitable for under hood automotive applications.ISO data provided by the manufacturer, Arkema.
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin
CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona..
Charpy Impact Unnotched 2.30 - 7.00 J/cm²
10.9 - 33.3 ft-lb/in²
Average value: 4.54 J/cm² Grade Count:41
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 2.30 J/cm²
10.9 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Copyright © lookpolymers.com All Rights Reserved