| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179 |
|
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -40.0 °C
|
21.4
ft-lb/in² <br>@Temperature -40.0 °F
|
DIN 53453 |
|
Nilit FRIANYL A63 TF-GV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass fiber reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/1U |
|
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -40.0 °C
|
21.4
ft-lb/in² <br>@Temperature -40.0 °F
|
DIN 53453 |
|
Nilit FRIANYL B63 W-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² - NB | 21.4 ft-lb/in² - NB | Average value: 9.06 J/cm² Grade Count:71 |
|
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 50-7164/BL02 Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Low warpag..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | |
|
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Lehmann & Voss LUVOCOM® 1/CF/30 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature -30.0 °C
|
21.4
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Lehmann & Voss LUVOCOM® 1105/GR/15/TF/15-2 PEEK, with PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | |
|
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/1eU |
|
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, DRY
Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Valox® 4012G PBT
VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East)
VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Valox® 420 PBT
30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors.
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 30.0 °C
|
21.4
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50
Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | dry; ISO 179/1eU |
|
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30
Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: ..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 30.0 °C
|
21.4
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30
Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following ..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 30.0 °C
|
21.4
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30
Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/1eU |
|
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based ..
|
|||
| Charpy Impact Unnotched |
4.50
J/cm² <br>@Temperature 30.0 °C
|
21.4
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30
Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation ..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179 |
|
BASF Ultramid® N-276 NF3001 40% Glass/Mineral Filled PA66 (Dry)
Ultramid N-276 NF3001 is a 40% mineral/glass reinforced, heat stabilized injection molding nylon 6/6.
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO179 |
|
Beijing Chemical Industry KAIFA® 301-G0F PBT Resin
Flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | Conditioned; ISO 179/IeU |
|
Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled
Glass fiber reinforced, high resistance to frictionInformation provided by Addiplast.
|
|||
| Charpy Impact Unnotched |
4.50
-
4.50
J/cm² <br>@Temperature -30.0 - -30.0 °C
|
21.4
-
21.4
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 4.50 J/cm² Grade Count:1 |
|
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
|
|||
| Charpy Impact Unnotched |
4.50
-
4.50
J/cm² <br>@Temperature -30.0 - -30.0 °C
|
21.4
-
21.4
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 4.50 J/cm² Grade Count:1 |
|
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
|
|||
| Charpy Impact Unnotched | 4.50 J/cm² | 21.4 ft-lb/in² | ISO 179/1eU |
|
CENTROPLAST CENTROCARB GF Polycarbonate 30% glass fiber
CENTROCARB GF is a transparent or semi-transparent plastic, reinforced for high strength and impact resistance. It has a high tensile modulus of elasticity and is well suited for structural element..
|
|||