| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched |
3.50
-
3.50
J/cm² <br>@Temperature -40.0 - -20.0 °C
|
16.7
-
16.7
ft-lb/in² <br>@Temperature -40.0 - -4.00 °F
|
Average value: 3.50 J/cm² Grade Count:1 |
|
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature -40.0 °C
|
16.7
ft-lb/in² <br>@Temperature -40.0 °F
|
DIN 53453 |
|
Nilit FRIANYL B63 GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature -40.0 °C
|
16.7
ft-lb/in² <br>@Temperature -40.0 °F
|
DIN 53453 |
|
Nilit FRIANYL B63 GV15 Nylon 6 for injection molding, 15% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | |
|
Arkema Group Oroglas® MI-4T Acrylic, Heat Resistant
(discontinued **)
OROGLAS MI-4T is an acrylic grade that associates improved impact resistance with high heat resistance.Key features improved impact resistance: up to 4 times more impact resistant than standard acr..
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² - NB | 16.7 ft-lb/in² - NB | Average value: 9.02 J/cm² Grade Count:124 |
|
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 1105-7290 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 1106-7033 Polyether imide, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature -30.0 °C
|
16.7
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Lehmann & Voss LUVOCOM® 1-7882 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | flatwise; ISO 179 1fU |
|
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature -30.0 °C
|
16.7
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Lehmann & Voss LUVOCOM® 50/CF/10/GF/10/TF/10/BK Polycarbonate, with carbon fiber, glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature -30.0 °C
|
16.7
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist..
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 1800-7519 PET, with carbon fiber, PTFE, mineral resin
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | |
|
LATI Latilub 66-10T K/10 PA66, 10% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | |
|
LATI Latilub 85-10T G/30 PES, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyether Sulfone (PES). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature -30.0 °C
|
16.7
ft-lb/in² <br>@Temperature -22.0 °F
|
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics ULTEM 2200R PEI (Europe-Africa-Middle East)
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | IS0179 |
|
Zhejiang Juner 301-G15 15% Glass Fibre Reinforced and Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature 23.0 °C
|
16.7
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eU |
|
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature 30.0 °C
|
16.7
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30
Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr..
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature 30.0 °C
|
16.7
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® GV-2 FWA nat PA*-GF20
Product description: Grivory GV-2 FWA natural is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyami..
|
|||
| Charpy Impact Unnotched |
3.50
J/cm² <br>@Temperature 30.0 °C
|
16.7
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® GV-2H PA*-GF20
Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide...
|
|||
| Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | ISO179 |
|
Beijing Chemical Industry KAIFA® 304-GO0 PBT Resin
Flame retardant, low bleeding, UV-resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Charpy Impact Unnotched |
3.50
-
4.00
J/cm² <br>@Temperature -30.0 - -30.0 °C
|
16.7
-
19.0
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 3.90 J/cm² Grade Count:5 |
|
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
|
|||
| Charpy Impact Unnotched | 3.50 - 8.00 J/cm² | 16.7 - 38.1 ft-lb/in² | Average value: 5.88 J/cm² Grade Count:4 |
|
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a..
|
|||