Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 HH-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 6.50 J/cm²

@Temperature -40.0 °C
30.9 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)  (discontinued **)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 80-7014 Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Grupo Repol Dinalon® B1X25 G30V0 PA6 30% Glass Fiber, V0 Red Phosphorus and Halogen Free
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179-1eU
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers
PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1-0889-4 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1-0936 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
LATI Latene® AG7H G/30 PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers. Good thermal propertiesAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179-1
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Conditioned
Information provided by Unitika Ltd.
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® AG-30 H PA66
Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor..
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® BG-35 PA6-GF35
Product description: Grilon BG-35 is a heat stabilized PA6 injection molding grade with 35% glass fibers. Grilon BG-35 has the following important properties: High stiffness Good surface finishEasy..
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® BG-40 HM PA6-GF40
Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15
Product description: Grilon EBGM-20 HX black 9992 is a high viscosity, high heat stabilized PA66 + PA6 extrusion blow molding grade with 15% glass fibers. The special features of Grilon EBGM-20 HX b..
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30
Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi..
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® LV-3 ESD PA12-GF30
Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Crastin® HR5330HF BK503 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40
Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Crastin® SK605 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 BK851 is a 30% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® BGK-30 X PA6-(GF+GB)30
Information provided by EMS Grivory
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® LBV-65H FWA nat PA12-GF65
Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Conditioned)
Ultramid 1403-2 NF3001 is a 13% glass reinforced, heat stabilized injection molding PA6/6.
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry)
Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6.
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® GVX-5 H black 9915 PA*-GF50
Product description: Grivory GVX-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 30.0 °C
30.9 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® GVX-5 H nat PA*-GF50
Product description: Grivory GVX-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
dry; ISO 179 1eU
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/IeU
Addiplast Addinyl C2 ZV40 Nylon 66/6, 40% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.