Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 33.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature -40.0 °C
33.3 ft-lb/in²
<br>@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL B63 HS-GV 5 Nylon 6 for injection molding, 5% glass fiber reinforced
Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature 23.0 °C
33.3 ft-lb/in²
<br>@Temperature 73.4 °F
Injection Molded; ISO 179
PolyOne Bergamid™ B70 G30 BK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Charpy Impact Unnotched 7.00 J/cm² - NB
<br>@Temperature -30.0 - -20.0 °C
33.3 ft-lb/in² - NB
<br>@Temperature -22.0 - -4.00 °F
Average value: 10.3 J/cm² Grade Count:26
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Charpy Impact Unnotched 7.00 - 12.0 J/cm²
<br>@Temperature -30.0 - -30.0 °C
33.3 - 57.1 ft-lb/in²
<br>@Temperature -22.0 - -22.0 °F
Average value: 8.60 J/cm² Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature 23.0 °C
33.3 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal &nbsp;(Unverified Data**)
Delrin® FG400MTD BLA079 is a metal filled, medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for consideration into applications such..
Charpy Impact Unnotched 7.00 - 7.50 J/cm²
<br>@Temperature -30.0 - -30.0 °C
33.3 - 35.7 ft-lb/in²
<br>@Temperature -22.0 - -22.0 °F
Average value: 7.17 J/cm² Grade Count:6
Overview of materials for Nylon 63, 35% Glass-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15 Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179
Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 0
Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.Colors: it is marketed in the natural and black color.Available in: Latin America Main Properties:..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179-1
Unitika M1030DH PA6, Conditioned
Nano composite nylonInformation provided by Unitika Ltd.
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature 30.0 °C
33.3 ft-lb/in²
<br>@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® BG-30 S FA PA6-GF30
Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy ..
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature 23.0 °C
33.3 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature 23.0 °C
33.3 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 MR 209 HWCP 20% Mineral Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature 30.0 °C
33.3 ft-lb/in²
<br>@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65
Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65
Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami..
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature 30.0 °C
33.3 ft-lb/in²
<br>@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35
Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature 30.0 °C
33.3 ft-lb/in²
<br>@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30
Product description: Grivory XE 4063 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50
Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® XE 4174 black 9992 PA1010-GF30
Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010..
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature -30.0 °C
33.3 ft-lb/in²
<br>@Temperature -22.0 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66 &nbsp;(Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
Charpy Impact Unnotched 7.00 J/cm²
<br>@Temperature 30.0 °C
33.3 ft-lb/in²
<br>@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60
Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
cond.; ISO 179 1eU
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
dry; ISO 179 1eU
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry)
Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6.
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned)
Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
cond.; ISO 179 1eU
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
Polimeri Europa SINKRAL PD G120 ABS &nbsp;(discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-09-30 General purpose injection moulding grade. Characteristics: outstanding rigidity very high surface..
Copyright © lookpolymers.com All Rights Reserved