| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | DIN 53453 |
|
Nilit FRIANYL A63 TF-GV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass fiber reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact Unnotched |
4.70
J/cm² @Temperature 23.0 °C |
22.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
|
Polykemi AB SCANAMID 66 A12^ F30 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Charpy Impact Unnotched |
4.70
J/cm² @Temperature -30.0 °C |
22.4
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Charpy Impact Unnotched |
4.70
J/cm² @Temperature -30.0 °C |
22.4
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Lexan® DMX3415M PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX3415M is a co-polycarbonate resin with improved scratch and abrasion resistance compared to standard polycarbonate. Lexan* DMX3415M is available in transparent colors.
|
|||
| Charpy Impact Unnotched |
4.70
J/cm² @Temperature -30.0 °C |
22.4
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Charpy Impact Unnotched | 4.70 - 7.00 J/cm² | 22.4 - 33.3 ft-lb/in² | Average value: 5.88 J/cm² Grade Count:5 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | Conditioned; ISO 179/1eU |
|
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
|
|||
| Charpy Impact Unnotched |
4.70
J/cm² @Temperature -30.0 °C |
22.4
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Charpy Impact Unnotched |
4.70
J/cm² @Temperature -30.0 °C |
22.4
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | |
|
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled |
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | |
|
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled |
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | |
|
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled. Used in Automotive and Industrial applications
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
|
|||
| Charpy Impact Unnotched |
4.70
J/cm² @Temperature -30.0 °C |
22.4
ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
|
Lehmann & Voss LUVOCOM® 1105/GN7348 PEEK, unreinforced, laser markable
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Not flammable.Especially suitable for medica..
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | flatwise; ISO 179 1fU |
|
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | ISO 179/1eU |
|
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned
Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications:..
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | ISO 179/1eU |
|
Solvay TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY
Description: TECHNYL® C 52G4 MZ25 is a 25% mineral reinforced melamine cyanurate flame retarded polyamide 6.This product is heat stabilized and is suitable for injection molding. This product is ..
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | Type 1, Edgewise; ISO 179 |
|
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
|
|||
| Charpy Impact Unnotched |
4.70
J/cm² @Temperature -30.0 °C |
22.4
ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics NORYL GFN3 PPE+PS
PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui..
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | ISO 179/1eU |
|
Borealis Nepol™ GB303HP 30% Long Glass Fiber Reinforced Polypropylene
Nepol GB303HP is a 30% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th..
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | ISO 179/1eU |
|
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced
Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st..
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | ISO 179/1eU |
|
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Information provided by BASF
|
|||
| Charpy Impact Unnotched |
4.70
J/cm² @Temperature 23.0 °C |
22.4
ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
|
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry)
Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain..
|
|||
| Charpy Impact Unnotched | 4.70 J/cm² | 22.4 ft-lb/in² | ISO 179/1eU |
|
BASF Ultrason E 2010 G4 20% Glass Filled PES
Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
|
|||