Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 6.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
PolyOne OnForce™ LFT PP-40LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
PolyOne OnForce™ LFT PP-40LGF/001 UV Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO Data
Americas Styrenics Styron® 6010 High Impact Polystyrene  (discontinued **)
STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac..
Charpy Impact Unnotched 6.00 J/cm² - NB
28.6 ft-lb/in² - NB
Average value: 12.5 J/cm² Grade Count:35
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Charpy Impact Unnotched 6.00 - 11.0 J/cm²
<br>@Temperature -30.0 - 30.0 °C
28.6 - 52.4 ft-lb/in²
<br>@Temperature -22.0 - 86.0 °F
Average value: 8.87 J/cm² Grade Count:24
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature -30.0 °C
28.6 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 1105/MS/15/TF/15 PEEK, with PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
LATI Latistat 47/7-03 PP Copolymer
Dissipative product based on Polypropylene copolymer (PPc). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter..
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature -30.0 °C
28.6 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/2C
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East)
VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature 23.0 °C
28.6 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 HW Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature 23.0 °C
28.6 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70
Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature 30.0 °C
28.6 ft-lb/in²
<br>@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45
Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST..
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature 30.0 °C
28.6 ft-lb/in²
<br>@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45
Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® LV-3 X ESD black PA12-GF30
Grilamid LV-3 X ESD black is an antistatic Polyamide 12 for injection molding with 30% glass fiber reinforcement. Main attributes are: antistatic with resistivity < 106 Ohmgood fuel and zinc chlorid..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® LV-65H FWA nat PA12-GF65
Product description: Grilamid LV-65H FWA natural is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature 30.0 °C
28.6 ft-lb/in²
<br>@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30
Information provided by EMS Grivory
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature 30.0 °C
28.6 ft-lb/in²
<br>@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30
Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab..
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature 23.0 °C
28.6 ft-lb/in²
<br>@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)
Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
Edgew 80x10x4 sp=62; ISO 179/1eU
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded
Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar.
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65
Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined..
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature 30.0 °C
28.6 ft-lb/in²
<br>@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65
Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179 1eU
Azoty Tarnow™ Tarnamid® T-27 MW30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
Conditioned; ISO 179/IeU
Addiplast Addinyl A2 ZG30 Nylon 66, 30% Glass Bead
Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast.
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
Conditioned; ISO 179/IeU
Addiplast Addinyl A2H V25 Flame Retardant Nylon 66, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast.
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
CENTROPLAST CENTRODAL MD Polyoxymethylene, Magnetically Detectable
During the modification with POM MD, metal fillings are added to the basic polyoxymethylene, which allows the plastic to be detectable. The excellent machinability, tenacity and dimensional stabilit..
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/IeU
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Charpy Impact Unnotched 6.00 J/cm²
<br>@Temperature 30.0 °C
28.6 ft-lb/in²
<br>@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TRVX-50X9 nat PAMACM12-GF50
Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and..
Copyright © lookpolymers.com All Rights Reserved