| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched |
6.50
J/cm² @Temperature 23.0 °C |
30.9
ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide..
|
|||
| Charpy Impact Unnotched |
6.50
J/cm² @Temperature -40.0 °C |
30.9
ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
|
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)
(discontinued **)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179 |
|
Lucite International Perspexâ„¢ XT IM60 Acrylic Impact Modified Extruded Sheet
PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | |
|
LATI Latamid 66 H2 G/50-GWHF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. improved G.W.F.I. compared to standard product.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | edgewise; ISO 179 1eU |
|
Lehmann & Voss LUVOCOM® 1105/XCF/25 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | |
|
LATI Latilub 66-01M G/30 PA66, 30% Glass Fiber Reinforced, Molybdenum disulphide Filled
Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | |
|
LATI Latilub 66-01M G/50 PA66, 50% Glass Fiber Reinforced, Molybdenum disulphide Filled
Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | |
|
LATI Latiohm 62-03 PD01 G/20 PPA, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eU |
|
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY
Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eU |
|
Solvay TECHNYL® A 238 V13 PA66, 13% glass fiber, DRY
Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.Available in: Europe, Latin America and North AmericaProduct Ap..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
|
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
|
|||
| Charpy Impact Unnotched |
6.50
J/cm² @Temperature 30.0 °C |
30.9
ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® BG-40 HM PA6-GF40
Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop..
|
|||
| Charpy Impact Unnotched |
6.50
J/cm² @Temperature 30.0 °C |
30.9
ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® LKN-5H PA12-GB50
Product description: Grilamid LKN-5H is a 50% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | dry; ISO 179/1eU |
|
EMS-Grivory Grivory® TSG-30/4 V0 PA666-GF30 FR
Product description: Grilon TSG-30/4 V0 is a heat stabilized, flame retardant, self-extinguishing engineering thermoplastic, reinforced with glass-fiber 30% (by weight) based on a semi-crystalline P..
|
|||
| Charpy Impact Unnotched |
6.50
J/cm² @Temperature 30.0 °C |
30.9
ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40
Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following ..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eU |
|
DuPont Performance Polymers Crastin® HR5330HF BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**)&
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
|
|||
| Charpy Impact Unnotched |
6.50
J/cm² @Temperature -30.0 °C |
30.9
ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
|
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eU |
|
DuPont Performance Polymers Crastin® SK605 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 BK851 is a 30% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
|
|||
| Charpy Impact Unnotched |
6.50
J/cm² @Temperature -30.0 °C |
30.9
ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | dry; ISO 179/1eU |
|
EMS-Grivory Grivory® LBV-65H FWA nat PA12-GF65
Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/1eU |
|
Pasargad Polymer Peyvand Pasamid 3P-M1130B Nylon 6, 30% Glass Fiber Reinforced
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
|
|||
| Charpy Impact Unnotched |
6.50
J/cm² @Temperature -30.0 °C |
30.9
ft-lb/in² @Temperature -22.0 °F |
|
|
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)
(discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI..
|
|||
| Charpy Impact Unnotched |
6.50
J/cm² @Temperature 30.0 °C |
30.9
ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® GVX-5 H black 9915 PA*-GF50
Product description: Grivory GVX-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | DAM; ISO 179/1eU |
|
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/IeU |
|
Addiplast Addinyl B2 V40 Nylon 6, 40% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/IeU |
|
Addiplast Addinyl B25 V25 Flame Retardant Nylon 6, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast.
|
|||
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | |
|
LATI Latilub 67-10STE21 G/20 PA66, 20% Glass Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66), impact modified. Silicone / PTFE. Toughened. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
|
|||