| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 4.70 - 7.00 J/cm² | 22.4 - 33.3 ft-lb/in² | Average value: 5.88 J/cm² Grade Count:5 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
|
|||
| Charpy Impact Unnotched | 2.20 - 7.00 J/cm² | 10.5 - 33.3 ft-lb/in² | Average value: 5.51 J/cm² Grade Count:17 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
|
|||
| Charpy Impact Unnotched | 2.00 - 7.00 J/cm² | 9.52 - 33.3 ft-lb/in² | Average value: 4.04 J/cm² Grade Count:13 |
|
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
|
|||
| Charpy Impact Unnotched |
2.50
-
7.00
J/cm² @Temperature -40.0 - 30.0 °C |
11.9
-
33.3
ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 4.64 J/cm² Grade Count:11 |
|
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
|
|||
| Charpy Impact Unnotched | 3.50 - 7.00 J/cm² | 16.7 - 33.3 ft-lb/in² | Average value: 5.62 J/cm² Grade Count:13 |
|
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Charpy Impact Unnotched |
3.00
-
7.00
J/cm² @Temperature -20.0 - 30.0 °C |
14.3
-
33.3
ft-lb/in² @Temperature -4.00 - 86.0 °F |
Average value: 4.40 J/cm² Grade Count:5 |
|
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
|
|||
| Charpy Impact Unnotched | 2.30 - 7.00 J/cm² | 10.9 - 33.3 ft-lb/in² | Average value: 4.54 J/cm² Grade Count:41 |
|
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Charpy Impact Unnotched |
2.00
-
7.00
J/cm² @Temperature -30.0 - -30.0 °C |
9.52
-
33.3
ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.27 J/cm² Grade Count:34 |
|
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Charpy Impact Unnotched | 2.70 - 7.00 J/cm² | 12.8 - 33.3 ft-lb/in² | Average value: 4.88 J/cm² Grade Count:13 |
|
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
|
|||
| Charpy Impact Unnotched | 2.30 - 7.00 J/cm² | 10.9 - 33.3 ft-lb/in² | Average value: 4.49 J/cm² Grade Count:27 |
|
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
|
|||