Polymer Property : Izod Impact, Unnotched = 0.932 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.932 J/cm
1.74 ft-lb/in
ASTM D256
Hyosung Topilene J640A PP
J640A Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporatio..
Izod Impact, Unnotched 0.932 - 9.60 J/cm
1.75 - 18.0 ft-lb/in
Average value: 6.00 J/cm Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Izod Impact, Unnotched 0.932 J/cm

@Thickness 3.17 mm
1.74 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Tripet® 2500G45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information..