Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 1.30 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Izod Impact, Unnotched 1.30 - 1.70 J/cm

@Temperature 23.0 °C
2.44 - 3.18 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKS 205/K Rigid PVC, Antishock Extrusion Lead Free
Metal effect antishock profiles
Izod Impact, Unnotched 1.30 - 1.70 J/cm

@Temperature 23.0 °C
2.44 - 3.18 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKS 205/K-UV Rigid PVC, Antishock Extrusion Lead Free
Metal effect antishock UV resistant profiles
Izod Impact, Unnotched 1.30 - 1.70 J/cm

@Temperature 23.0 °C
2.44 - 3.18 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKS 325/W-UV Rigid PVC, Antishock Extrusion Lead Free
Various profiles, antishock UV resistant
Izod Impact, Unnotched 1.30 - 1.70 J/cm

@Temperature 23.0 °C
2.44 - 3.18 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKT 226 Rigid PVC, Extrusion Lead Free
Metal effect profiles
Izod Impact, Unnotched 1.30 - 1.70 J/cm

@Temperature 23.0 °C
2.44 - 3.18 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKT 736/K1 Rigid PVC, Extrusion Lead Free
Transparent profiles
Izod Impact, Unnotched 1.30 J/cm
2.44 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOTUF CF007IXP PS
LNP* Thermotuf* CF007IXP is a compound based on Polystyrene containing glass fiber. Characteristics of this grade are: High Impact.
Izod Impact, Unnotched 1.30 - 1.70 J/cm

@Temperature 23.0 °C
2.44 - 3.18 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds ARC 10 Rigid PVC, Atoxic for General Purpose
Bottles medium antishock
Izod Impact, Unnotched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
ALM PA 605-A Filled Nylon 12 Prototyping Polymer
50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a..
Izod Impact, Unnotched 1.30 - 1.70 J/cm

@Temperature 23.0 °C
2.44 - 3.18 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKT 736 Rigid PVC, Extrusion Lead Free
Transparent antishock profiles